综述了第一代耐316℃聚酰亚胺的研究发展状况,对该类材料的化学结构、组成、制备以及结构与性能之间的关系等进行了介绍.

参考文献

[1] Meador MA. .Recent advances in the development of processable high-temperature polymers [Review][J].Annual review of materials research,1998(0):599-630.
[2] 陈祥宝.先进树脂基复合材料的发展[J].航空材料学报,2000(01):46-54.
[3] 谭必恩,益小苏.航空发动机用PMR聚酰亚胺树脂基复合材料[J].航空材料学报,2001(01):55-62.
[4] Wilson D .PMR-15 processing,properties and problems-a review[J].British Polymer Journal,1988,20(05):405-416.
[5] Stenzenberger H .Recent advances in thermosetting polyimides[J].British Polymer Journal,1988,20(05):383-396.
[6] Pater R H .Thermosetting polyimides:A review[J].SAMPE Journal,1994,30(05):29-38.
[7] Zhou J.;Liu WL.;Ding MX.;He TB.;Zhang J. .THE EFFECT OF FORMULATED MOLECULAR WEIGHT ON TEMPERATURE RESISTANCE AND MECHANICAL PROPERTIES IN POLYIMIDE BASED COMPOSITES[J].Journal of Materials Science,1996(19):5119-5125.
[8] Malarik D C;Vannucci R D .High molecular weight first generation PMR polyimides for 343℃ applications[J].SAMPE Quarterly,1992,23(04):3-8.
[9] Chuk L.Leung;Reza Ghaffarian;Kenneth C.Leung .Thermo-oxidative stability of polyimides-I effect of prepolymer molecular weights[J].Polymer Degradation and Stability,1997(1/2):11-14.
[10] Meador MAB.;Cavano PJ.;Johnston JC. .ELUCIDATION OF THE CROSS-LINK STRUCTURE OF NADIC-END-CAPPED POLYIMIDES USING NMR OF C-13-LABELED POLYMERS[J].Macromolecules,1997(3):515-519.
[11] Meador MAB.;Cavano PJ.;Frimer AA.;Johnston JC. .OXIDATIVE DEGRADATION OF NADIC-END-CAPPED POLYIMIDES .2. EVIDENCE FOR REACTIONS OCCURRING AT HIGH TEMPERATURES[J].Macromolecules,1997(11):3215-3223.
[12] Bowles K J .Longtime durability of PMR-15 matrix polymer at 204,260,288 and 316℃[Z].NASA Technical Memorandum,n 210602,2001.
[13] Bowles K J;Jayne D;Leonhardt T A .Thermal stability relationships between PMR-15 resin and its composites[J].Journal of Advanced Materials,1994,26(01):23-32.
[14] Scola D A;Vontell J H .Mechanical properties and mechanism of the degradation process of 316℃ Isothermally aged graphite fiber/PMR-15 composites[J].Polymer Engineering and Science,1991,31(01):6-13.
[15] Bowles K J .Effect of fiber reinforcements on thermooxidative stability and mechanical properties of polymer matrix composites[J].SAMPE Quarterly,1992,23(03):2-12.
[16] Bowles K J .Effects of fiber surface modification and thermal aging on composite toughness and its measurement[Z].NASA Technical Memorandum,n 106765,1995.
[17] Tsuji L C;McManus H L;Bowles K J .Mechanical properties of degraded PMR-15 resin[Z].NASA Technical Memorandum,n 208487,1998.
[18] Lili L.Johnson;R.K.Eby;Mary Ann B.Meador .Investigation of oxidation profile in PMR-15 polyimide using atomic force microscope (AFM)[J].Polymer: The International Journal for the Science and Technology of Polymers,2003(1):187-197.
[19] Simone CD;Xiao YM;Sun XD;Scola DA .Some aspects of the cure of RP-46, a nadic end-capped polyimide, and phenyl nadimide and bis-nadic-3,4 '-ODA model compounds[J].High performance polymers,2005(1):51-72.
[20] Yumin Liu;Y.Xiao;X.Sun;D.A.Scola .Microwave Irradiation of Nadic-End-Capped Polyimide Resin (RP-46) and Glass-Graphite-RP-46 Composites: Cure and Process Studies[J].Journal of Applied Polymer Science,1999(12):2391-2411.
[21] Badir A;Shonkwiler B;Brawley J P.Fatigue testing of unidirectional T650-35/AMB 21 laminates[A].,1998
[22] R. A. Gray;L. R. McGrath .The Development of High-Temperature Polyimides for Resin Transfer Molding[J].SAMPE Journal,2004(6):23-31.
[23] Delvigs P;Klopotek D L;Cavano P J .Structure-property relationships in addition polyimides.Ⅱ.Resins from threering aromatic diamines containing carbonyl and methylene groups[J].High Performance Polymers,1997,9(02):161-176.
[24] Chnang K C .High Tg PMR polyimides[R].NASA report 20000056866
[25] Matsuura T;Yamada N;Nishi Y .Polyimides derived from 2,2'-bis (trifiuoromethyl) -4,4'-diaminobiphenyl.3.Property control for polymer blends and copolymerization of fluorinated polyimides[J].Macromolecules,1993,26(03):419-423.
[26] Xie W;Chuang K C .Thermal degradation study of polymerization of monomeric reactants (PMR) polymides[J].Journal of Thermal Analysis and Calorimetry,2001,64(02):477-485.
[27] Chuang K C;Vannucci R D;Ansari I .High flow addition curing polymers[J].Journal of Polymer Science Part A:Polymer Chemistry,1994,32(07):1341-1350.
[28] Chuang K C .Polyimides based on 2,2 prime,6,6prime tetramethylbenzidine[J].High Performance Polymers,1995,7(01):81-92.
[29] Kathy C. Chuang;Kenneth J. Bowles;Demetrious S. Papadopoulos .A High T_g PMR Polyimide Composites (DMBZ-15)[J].Journal of advanced materials,2001(4):33-38.
[30] Steven P;James P.Tough,processable,non-MDA polyimide[A].,1999:96-102.
[31] Pater R H .Dynamic mechanical properties of N-phenylnadimide modified PMR polyimide composites[J].Polymer Composites,1991,12(02):133-136.
[32] Pater R H .371℃ (700F) propertiesofcelion6000/N-phenylnadimide modified PMR polyimide composites[J].Polymer Engineering and Science,1991,31(01):14-19.
[33] T J Xiao;S Q Gao;A J Hu;X C Wang;S Y Yang .Thermosetting polyimides with improved impact toughness and excellent thermal and thermo-oxidative stability[J].High performance polymers,2001(4):287-299.
[34] 陈建升 .高性能聚酰亚胺基体树脂及其复合材料的研究[D].北京:中国科学院,2005.
[35] Fang X Z;Wang Z;Ding M X .Novel polyimides derived from 2,3,3,4-benzophenonetetracarboxylic[J].Dianhydride Polymer,2003,44(09):2641-2646.
[36] Li X G;Xiong L;Yi X S .Toughness improvement of PMtR-type polyimide and laminated graphite systems by ex-situ concept[J].Journal of Materlials Science,2005,40(18):5067-5070.
[37] Zhang Z G;Li M;Pan Y S .Thermal properties of novel PMR polyimides prepared by eopolymerization[J].Polymers and Polymer Composites,2004,12(05):399-408.