综述了国内外推进剂材料老化性能的研究进展.介绍了推进剂材料老化所采用的光谱法、色谱法、热分析法、传感器法、凝胶溶胶法、动态粘弹法等.展望了该研究领域未来的发展趋势,以光谱学和在推进剂中埋入微型传感器等老化无损评估方法是该领域今后的主要发展方向.
参考文献
[1] | 肖琰,魏伯荣,杜茂平.橡胶加速老化试验及贮存期推算方法[J].合成材料老化与应用,2007(01):40-43. |
[2] | 张长生,王建华,石耀刚,丁国芳.聚氨酯耐热降解性能的研究进展[J].合成材料老化与应用,2005(02):28-32. |
[3] | 邹德荣.聚醚聚氨酯弹性体及其老化性能研究[J].合成材料老化与应用,2002(02):13-18. |
[4] | Sridhar BTN;Ravichandran K;Nagappa R.Study of ageing behaviour of a composite solid propellant using mechanical and ballistic tests[A].Karlsruhe,Germany,2006 |
[5] | Jeunieau L;Lefebvre MH;Guillaume P.Chemical and ballistic stability analyses of rolled ball propellants[A].Karlsruhe,Germany,2006 |
[6] | Keizers HLJ;Schadow KC.AVT-119,NATO health monitoring of munitions cooperative demonstration of technology[A].Karlsruhe,Germany,2006 |
[7] | Bohn MA .Prediction of life times of propellants-improved Kinetic description of stabilizer consumption[J].Propellants,Explosives,Pyrotechnics,1994,19(05):266-269. |
[8] | Pearson L H;Doyle T E;Hamilton R S et al.The role of NDE in service life prediction of solid rocket propellant[AD-A330303][R].,1996. |
[9] | Tokui H;Iwama A .Aging Characteristics of Hydroxy-Terminated Polybutadiene Propellant[J].Kayaku Gakkaishi,1991,52(02):100-107. |
[10] | Chevalier S;Perut C;Billon L.Antioxidant Selection Methodology for Hydroxy-Terminated Polybuadiene Type Solid Propellants[A].Karlsruhe,Germany,1994 |
[11] | Dylan J. Nagle;Mathew Celina;Llewellyn Rintoul;Peter M. Fredericks .Infrared microspectroscopic study of the thermo-oxidative degradation of hydroxy-terminated polybutadiene/isophorone diisocyanate polyurethane rubber[J].Polymer Degradation and Stability,2007(8):1446-1454. |
[12] | Stephens W D;Schwarz W W;Kruse R B et al.Application of fourier transform spectroscopy to propellant service life prediction[AIAA 76748][R].,1976. |
[13] | Judge MD .The application of near-infrared spectroscopy for the quality control analysis of rocket propellant fuel pre-mixes[J].Talanta,2004,62(04):675-679. |
[14] | Robert Feigley;Feng Jin;Jose Lorenzo.Monitoring of chemical degradation in propellants using AOTF spectrometer[A].,2004:96-103. |
[15] | Bohn M A .Prediction of life times of propellants-improved Kinetic description of stabilizer consumption[J].Propellants,Explosives,Pyrotechnics,1994,19(05):266-269. |
[16] | Celina M;Elliott JMS;Winters ST;Assink RA;Minier LM .Correlation of antioxidant depletion and mechanical performance during thermal degradation of an HTPB elastomer[J].Polymer Degradation and Stability,2006(8):1870-1879. |
[17] | Ellison D S;Weemes C L.The assessment of the performance of medium caliber munitions during aging as a function of thermal stability,molecular weight and chamber pressure[A].Karlsruhe,Germany,2006 |
[18] | John MB;Paul RD;Philip PG.Whole life assessment of nitrocellulose in double base rocket propellants[A].Karlsruhe,Germany,2006 |
[19] | Whipple R .Field Analysis of Propellant Stabilizers and their Daughter Products in any Propellant Formulation by Thin-Layer Chromatography Year End Report 2003[UCRL-TR-201359][R].,2003. |
[20] | Wilken J.The qualitative analysis of explosives by means of Thin-Layer Chromatography (TLC)[A].Karlsruhe,Germany,2006 |
[21] | Pettersson M-L;Eldster C.Stability study of smokeless propellants of up to 60 years of age as measured by Heat Flow Calorimetry[A].Karlsruhe,Germany,2006 |
[22] | Deacon P;Garman R.Non-isothermal ageing of nitrocellulose based PBX compositions[A].Karlsruhe,Germany,2006 |
[23] | Little R R;Chelner H;Buswell H J.Development,testing and application of embedded sensors for solid rocket motor health monitoring[A].Karlsruhe,Germany,2006 |
[24] | Buswell J;Chelner H.Advances in embeddable sensors for health monitoring of solid rocket grains[A].Karlsruhe,Germany,2006 |
[25] | Johnson J L.Data collection requirements for quality evaluation (aging analysis) of energetic materials and methods[A].Karlsruhe,Germany,2006 |
[26] | Jimmy D C;Seema S;Darryl Y S et al.Autonomous optical sensor system for the monitoring of nitrogen dioxide from aging rocket propellant[SAND 2001-2953][R].,2001. |
[27] | Layton L H .Chemical structural aging studies on HTPB propellant[ADA010731][R].,1975. |
[28] | Layton L H .Chemical structural aging effects[ADA 002836][R].,1974. |
[29] | Cunliffe AV;Tod QinetiQ DA;Sevenoaks GB.Sol Fraction Measurements-A tool to study cross-linking and ageing in composite propellants and PBXs[A].Karlsruhe,Germany,2006 |
[30] | Neviere R;Guyader M.DMA:a powerful technique to assess ageing of MED[A].Karlsruhe,Germany,2006 |
[31] | Husband DM .Use of dynamic mechanical measurements to determine the aging behavior of solid propellant[J].Propellants,Explosives,Pyrotechnics,1992,17(04):196-201. |
[32] | Duncan EJS. .CHARACTERIZATION OF A GLYCIDYL AZIDE POLYMER COMPOSITE PROPELLANT - STRAIN RATE EFFECTS AND RELAXATION RESPONSE[J].Journal of Applied Polymer Science,1995(3):365-375. |
[33] | Duncan EJS.;Brousseau P. .COMPARISON OF THE UNIAXIAL TENSILE MODULUS AND DYNAMIC SHEAR STORAGE MODULUS OF A FILLED HYDROXY-TERMINATED POLYBUTADIENE AND GAP PROPELLANT[J].Journal of Materials Science,1996(5):1275-1284. |
[34] | 罗善国,陈福泰,罗运军,谭惠民,满光磊,郭燕文,张建国.推进剂组分对聚醚聚氨酯粘合剂热氧降解的影响(Ⅰ)硝酸酯增塑剂的影响[J].推进技术,1999(02):88-94. |
[35] | 罗善国,陈福泰,罗运军,谭惠民,满光磊,郭燕文,张建国.推进剂组分对聚醚聚氨酯粘合剂热氧降解的影响(Ⅱ)固体填料和助剂的影响[J].推进技术,1999(03):95-99. |
[36] | 罗善国,谭惠民,陈福泰,罗运军,仇武林,多英全.新型推进剂中聚氨酯粘合剂的稳定研究[J].推进技术,1999(06):100-105. |
[37] | 张昊,彭松,庞爱民,杜锡娟.NEPE推进剂老化过程中结构与力学性能的关系[J].火炸药学报,2007(01):13-16. |
[38] | 丁汝昆,唐承志.丁羟推进剂加速老化中动态弹性模量与力学性能的变化[J].推进技术,1998(03):86-88. |
[39] | 王春华,彭网大,翁武军,张仁.HTPB推进剂凝胶分解特性与老化性能的相关性[J].推进技术,2000(02):84-87. |
[40] | 张昊,庞爱民,彭松.固体推进剂贮存寿命非破坏性评估方法(Ⅰ)--老化特征参数监测法[J].固体火箭技术,2005(04):271-275. |
[41] | 张昊,庞爱民,彭松.固体推进剂贮存寿命非破坏性评估方法(Ⅱ)--动态力学性能主曲线监测法[J].固体火箭技术,2006(03):190-194,199. |
[42] | 朱智春.固体火箭发动机寿命预估的一种考虑[J].推进技术,1996(04):10. |
[43] | 朱智春,蔡峨.聚氨酯推进剂的温度湿度老化有限元分析[J].推进技术,1997(04):80-83. |