热、氧、臭氧、光等环境因素对橡胶制品的老化起到了加速作用,介绍了近年来橡胶老化机理的研究以及橡胶老化研究的实验方法和仪器分析方法.

参考文献

[1] 化学工业部合成材料老化研究所.高分子材料老化与防老化[M].北京:化学工业出版社,1979
[2] 杨清芝.现代橡胶工艺学[M].北京:中国石化出版社,1997
[3] 范刚.车用橡胶制品老化问题研究[J].汽车科技,2003(01):16-17,27.
[4] 朱绪飞,文威,贾红兵,刘霖.电容器密封橡胶及其老化机理[J].弹性体,2002(01):58-62.
[5] 侯婷婷,钟杰平,李程鹏,杨磊,李思东,白羽.天然橡胶和胶清橡胶的热氧降解特性研究[J].广州化工,2006(06):32-33.
[6] Naba K Dutta;D K Tripathy .The influence of curing systems on the properties of bromobutyl rubber:Part 2-Effect of concentration of curing resin on the dynamic mechanical properties[J].Polymer Degradation and Stability,1990,30(02):231-256.
[7] Garbarczyk M.;Kuhn W.;Klinowski J.;Jurga S. .Characterization of aged nitrile rubber elastomers by NMR spectroscopy and microimaging[J].Polymer: The International Journal for the Science and Technology of Polymers,2002(11):3169-3172.
[8] 刘洪涛,张华,向明,刘晓洪.ENR、MG塑炼胶的热氧老化性能研究[J].合成材料老化与应用,2007(01):5-7.
[9] 张北龙,刘惠伦.环氧化天然橡胶/PVC共混物的热氧降解[J].橡胶工业,2001(06):330-333.
[10] 付秋兰,吴向荣,温茂添.缩合型室温硫化硅橡胶耐热性的研究进展[J].有机硅材料,2003(01):28-31.
[11] 谢择民;李其山;王金亭.改进硅橡胶耐热性的研究[J].特种橡胶制品,1981(02):l.
[12] RADHAKRISHNAN T.S. .New Method for Evaluation of Kinetic Parameters and Mechanism of Degradation from Pyrolysis-GC Studies: Thermal Degradation of Polydimethylsiloxanes[J].Journal of Applied Polymer Science,1999(3):441-450.
[13] Grassie N;Macfarlane I G .The thermal degradation of polysiloxanes(I):Poly(dimethyl siloxane)[J].European Polymer Journal,1978,14(11):875.
[14] Grassie N;Macfarlane I G;Francey K F .The thermal degradation of polysiloxanes(II):Poly(methyl henylsiloxane)[J].European Polymer Journal,1979,15(05):415.
[15] Deshpande G;Rezac M E .The effect of phenyl content on the degradation of poly(dimethyldipheny1)siloxane copolymers[J].Polymer Degradation and Stability,2001,74(02):363.
[16] 张凯,范敬辉,吴菊英,马艳.硅橡胶泡沫材料的热氧老化机理研究[J].合成材料老化与应用,2007(03):18-21.
[17] 程买增,胡新嵩,莫万奎.室温硫化硅橡胶耐热性的研究进展[J].有机硅材料,2006(01):38-41.
[18] M.Patel;A.R.Skinner .Thermal ageing studies on room-temperature vulcanised polysiloxane rubbers[J].Polymer Degradation and Stability,2001(3):399-402.
[19] M. Abdul Kader;Anil K. Bhowmick .Thermal ageing, degradation and swelling of acrylate rubber, fluororubber and their blends containing polyfunctional acrylates[J].Polymer Degradation and Stability,2003(2):283-295.
[20] Goga NO;Demco DE;Kolz J;Ferencz R;Haber A;Casanova F;Blumich B .Surface UV aging of elastomers investigated with microscopic resolution by single-sided NMR[J].Journal of magnetic resonance,2008(1):1-7.
[21] 齐藤孝臣 .各种橡胶的老化机理[J].橡胶参考资料,1996,26(06):9-20.
[22] 陈舜娥.橡胶的大气老化[J].合成材料老化与应用,2003(01):34-38,49.
[23] 王作龄.防老剂应用技术[J].世界橡胶工业,2001(01):55-59.
[24] 江畹兰 .周期性形变及臭氧对橡胶寿命的影响[J].世界橡胶工业,1999,26(04):33-34.
[25] Radhakrishnan CK;Alex R;Unnikrishnan G .Thermal, ozone and gamma ageing of styrene butadiene rubber and poly(ethylene-co-vinyl acetate) blends[J].Polymer Degradation and Stability,2006(4):902-910.
[26] 陈经盛.橡胶老化防护与监测(一)[J].化工标准化与质量监督,1996(01):30-32.
[27] 张友南,杨军,陈忠海.天然橡胶制品抗疲劳性能的因素简析[J].世界橡胶工业,2002(06):35-39.
[28] 王梦蛟.橡胶工业手册第二分册[M].北京:化学工业出版社,1989:172.
[29] Visser S A;Hewitt C E;Binga T D .Stability of filled poly(diphenylsiloxane-co-dimethylsilOxane)elastomers to cyclic stress at elevated temperatu re[J].J Polym Sci(Part B):Polym Phys,1996,34(09):1679.
[30] 李青山,王新伟,殷永传.硅橡胶氟橡胶及其共混物阻燃热稳定和耐热油性的研究[J].世界橡胶工业,2005(02):40-44.
[31] Mohammadreza Mofidi;Elisabet Kassfeldt;Braham Prakash .Tribological behaviour of an elastomer aged in different oils[J].Tribology International,2008(9/10):860-866.
[32] Van der Waal G.The relationship between the chemical structure of ester base fluids and their influence on elastomer seals,and wear characteristics[J].Journal of Synthetic Lubrication,1984(1-4):35-47.
[33] M. Torbacke;A. Johansson .Seal Material and Base Fluid Compatibility: An Overview[J].Journal of Synthetic Lubrication,2005(2):123-142.
[34] 刘新民,吴霞.SBS基热塑性弹性体的老化性能研究[J].弹性体,2003(05):16-20.
[35] 肖琰,魏伯荣.天然橡胶硫化胶的热氧老化性研究[J].合成材料老化与应用,2006(02):21-23,54.
[36] 彭政 .氯化天然橡胶的热降解研究[D].华南热带农业大学,2001.
[37] 何兰珍,郭璇华,杨磊,钟杰平.气氛对低氮天然橡胶热降解的影响[J].应用化工,2004(02):7-10.
[38] 肖琰,魏伯荣,杨海涛,闫刚.几种分析技术在硫化胶热老化研究中的应用[J].橡胶工业,2006(12):754-757.
[39] 肖琰,魏伯荣,杜茂平.橡胶加速老化试验及贮存期推算方法[J].合成材料老化与应用,2007(01):40-43.
[40] 李永清,晏欣,郑淑贞.硫化橡胶防老化涂层的研制[J].合成材料老化与应用,2004(04):31-35.
[41] Brown RP.;Soulagnet G. .Microhardness profiles on aged rubber compounds[J].Polymer Testing,2001(3):295-303.
[42] Patel M;Skinner AR;Maxwell RS .Sensitivity of condensation cured polysiloxane rubbers to sealed and open-to air thermal ageing regimes[J].Polymer Testing,2005(5):663-668.
[43] Morrell PR.;Patel M.;Skinner AR. .Accelerated thermal ageing studies on nitrile rubber O-rings[J].Polymer Testing,2003(6):651-656.
[44] Bauer DR;Baldwin JM;Ellwood KR .Rubber aging in tires. Part 2: Accelerated oven aging tests[J].Polymer Degradation and Stability,2007(1):110-117.
[45] Deng Huang;Bart J.LaCount;Jose M.Castro .Development of a service-simulating accelerated aging test method for exterior tire rubber compounds I. Cyclic aging[J].Polymer Degradation and Stability,2001(2):353-362.
[46] LaCount BJ.;Castro JM.;Ignatz-Hoover F. .Development of a service-simulating, accelerated aging test method for exterior tire rubber compounds II. Design and development of an accelerated outdoor aging simulator[J].Polymer Degradation and Stability,2002(2):213-227.
[47] Kenneth T. Gillen;Mathew Celina;Robert Bernstein .Validation of improved methods for predicting long-term elastomeric seal lifetimes from compression stress-relaxation and oxygen consumption techniques[J].Polymer Degradation and Stability,2003(1):25-35.
[48] 刘振海.热分析导论[M].北京:化学工业出版社,1991
[49] Yu HP;Li SD;Zhong HP;Xu K .Studies of thermooxidative degradation process of chlorinated natural rubber from latex[J].Thermochimica Acta: An International Journal Concerned with the Broader Aspects of Thermochemistry and Its Applications to Chemical Problems,2004(1/2):119-124.
[50] Aji P. Mathew;S. Packirisamy;Sabu Thomas .Studies on the thermal stability of natural rubber/polystyrene interpenetrating polymer networks; thermogravimetric analysis[J].Polymer Degradation and Stability,2001(3):423-439.
[51] Kader M A;Bhowmick A K .Thermal aging,degradation and swelling of acrylate rubber,fluororubber and their blends containing polyfunctional acrylates[Q].Polymer Degradation and Stability,2003,79(02):283-295.
[52] 黄华明,陈美,曾宗强,张北龙.用TG、DTA研究不同品系天然橡胶热降解[J].热带农业工程,2006(02):35-37.
[53] 侯婷婷,李程鹏,钟杰平,杨磊,李思东.氯化钙凝固天然橡胶的热分析研究[J].广东化工,2006(11):26-28.
[54] Sirait K T;Suwarno S.Evaluation of surface degradation of silicone rubber under natural tropical aging using thermogravimetric and thermomechanical analysis[A].Xian:Institute of Electrical and Electronics Engineers Inc,2000:645-648.
[55] Wei YT;Nasdala L;Rothert H;Xie Z .Experimental investigations on the dynamic mechanical properties of aged rubbers[J].Polymer Testing,2004(4):447-453.
[56] Xie ZM;Wei YT;Liu YY;Du XW .Dynamic mechanical properties of aged filled rubbers[J].Journal of Macromolecular Science. Physics,2004(4):805-817.
[57] Wei YT;Nasdala L;Rothert H;Xie Z .Experimental investigations on the dynamic mechanical properties of aged rubbers[J].Polymer Testing,2004(4):447-453.
[58] Patel M;Morrell PR;Evans J .Load bearing property testing of a silica filled room temperature vulcanised polysiloxane rubber[J].Polymer Testing,2004(5):605-611.
[59] 张苹,兰惠萍,唐学明.1,2-聚丁二烯硫化胶的热氧老化性能及其防护体系的研究[J].高分子材料科学与工程,1989(06):55-60.
[60] Denardin E I G;Janissek P R .Samios n Time-temperature dependence of the thermo-oxidative aging of polychloroprene rubber[J].Thermochimica Acta,2003,395(02):159-167.
[61] 赵霞,张雪芹,黄铃,孙良.同步热分析法研究聚丁二烯橡胶热降解过程[J].橡胶工业,2006(06):370-372.
[62] Somers AE.;Burgar MI.;Forsyth M.;Hill AJ.;Bastow TJ. .Quantifying rubber degradation using NMR[J].Polymer Degradation and Stability,2000(1):31-37.
[63] Parker DD.;Koenig JL. .Solid-state C-13-NMR studies of changes in crosslinked carbon structure of natural rubber during heating under air and nitrogen environments[J].Journal of Applied Polymer Science,1998(7):1371-1383.
[64] Knorgen M;Heuert U;Schneider H;Barth P;Kuhn W .Spatially resolved and integral NMR investigation of the aging process of carbon black filled natural rubber[J].Polymer bulletin,1997(1):101-108.
[65] J.Y.Buzare;G.Silly;J.Emery;G.Boccaccio;E.Rouault .Aging effects on vulcanized natural rubber studied by high resolution solid state ~13C-NMR[J].European Polymer Journal,2001(1):85-91.
[66] Garbarczyk M.;Kuhn W.;Klinowski J.;Jurga S. .Characterization of aged nitrile rubber elastomers by NMR spectroscopy and microimaging[J].Polymer: The International Journal for the Science and Technology of Polymers,2002(11):3169-3172.
[67] Goga NO;Demco DE;Kolz J;Ferencz R;Haber A;Casanova F;Blumich B .Surface UV aging of elastomers investigated with microscopic resolution by single-sided NMR[J].Journal of magnetic resonance,2008(1):1-7.
[68] Rui Resendes;William Hopkins;Tony Niziolek;Wilfried Braubach .Cost-effective modifiers for the preparation of BIIR based tire tread formulations[J].Rubber World: The Technical Service Magazine for The Rubber Industry,2003(6):46-51.
[69] Kumar A;Commereuc S;Verney V .Aging of elastomers:a molecular approach based on rheological chamcterization[J].Polymer Degradation and Stability,2004,85(02):751 757.
[70] 李思东;彭政;余和平 等.用红外差谱表征橡胶的热老化[J].橡胶工业,1998,45(08):494-498.
[71] 钱红莲,王平粤,陈鹰.老化对环氧化天然橡胶分子结构及性能的影响[J].应用化学,2005(10):1152-1154.
[72] 张静芳.增塑溴化丁基橡胶撕裂断裂及拉伸断裂的扫描电镜观察[J].橡胶译丛,1992(04):71-76.
[73] N. Dadvand;R.S. Lehrle;I.W. Parsons .Use of pyrolysis-GC-MS to assess the thermal degradation behaviour of polymers containing chlorine II. Thermal stability characteristics of Neoprene/chlorobutyl rubber composites, before and after artificial ageing[J].Polymer Degradation and Stability,2000(3):407-419.
[74] F. Delor-Jestin;J. Lacoste;N. Barrois-Oudin .Photo-, thermal and natural ageing of ethylene-propylene-diene monomer (EPDM) rubber used in automotive applications. Influence of carbon black, crosslinking and stabilizing agents[J].Polymer Degradation and Stability,2000(3):467-477.
[75] 魏小琴,余淑华,许明,何建新.用X射线光电子能谱法研究氟硅橡胶的热氧老化机理[J].橡胶工业,2008(07):441-443.
[76] Mpate1 .Aging and characterization of polysiloxane rubbers[J].Aging Studies and Lifetime Extension of Materials,1999,36(01):97-10l.
[77] A.N.Chaudhry;N.C.Billingham .Characterisation and oxidative degradation of a room-temperature vulcanised poly(dimethylsiloxane)rubber[J].Polymer Degradation and Stability,2001(3):505-510.
[78] Do TT.;Celina M.;Fredericks PM. .Attenuated total reflectance infrared micro spectroscopy of aged carbon-filled rubbers[J].Polymer Degradation and Stability,2002(3):417-422.
[79] Zhu, Y;Otsubo, M;Honda, C;Tanaka, S .Loss and recovery in hydrophobicity of silicone rubber exposed to corona discharge[J].Polymer Degradation and Stability,2006(7):1448-1454.
[80] Nsouli B.;Roumie M.;Zahraman K.;Thomas JP.;Jaksic M.;Pastuovic Z. Dole P.;Nasreddine M. .PIXE, micro-PIXE and RBS analysis of thermal aged rubber material: On the additives behaviour versus aging time[J].Nuclear Instruments and Methods in Physics Research, Section B. Beam Interactions with Materials and Atoms,2002(3/4):201-207.
[81] Fulton WS.;Smith GC.;Titchener KJ. .Interfacial microanalysis of rubber-tyre-cord adhesion and the influence of cobalt[J].Applied Surface Science: A Journal Devoted to the Properties of Interfaces in Relation to the Synthesis and Behaviour of Materials,2004(1/4):69-86.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%