本文综合介绍Ti3SiC2的最新研究进展.三元碳化物Ti3SiC2属于层状六方晶体结构,空间群为P63/mmC;它同时具有金属和陶瓷的优良性能,有良好的导电和导热能力,高弹性模量和低维氏显微硬度,在室温下可切削加工,在高温下能产生塑性变形,良好的高温热稳定性和优秀的抗氧化性能;应用CVD、SHS、HP/HIP等方法可制备该化合物,用HIP方法能制备高纯、致密的Ti3SiC2陶瓷;Ti3SiC2陶瓷材料自身有抵抗损伤的机理.

参考文献

[1] Jeitschlo;H Nowotny.Ein Neuer Komplexcarbid-Typ[J].Monatshefte Fur Chemie,1967(29)
[2] E H Kisi;J A A Crosslwy;S Myhra;M W. Barsoum .[J].Journal of Physics and Chemistry of Solids,1998,59(09):1437.
[3] M Amer;I Weiss;S Leelair;D Liptak .[J].Journal of Applied Physics,1998,84(10):5817.
[4] T Goto;T Hirai.[J].Materials Research Bulletin,1987(22):1195.
[5] R Pampuch;J Lis;L Stobierski;M Tymkiewiez.[J].Journal of the European Ceramic Society,1989(05):283.
[6] R Pampuch;J Lis;J Piekarczyk;L stobierski.[J].Journal of Materials Synthesis and Processing,1993(01):93.
[7] J. Lis;Y. Miyamoto;R. Pampuch .Ti_3SiC-based materials prepared by HIP-SHS techniques[J].Materials Letters,1995(3/4):163-168.
[8] Michel W;Barsoum;Tamer EI-Raghy .[J].Journal of the American Ceramic Society,1996,19(07):1953.
[9] Tamer EI-Raghy;Michel W .Barsoum[J].Journal of the American Ceramic Society,1999,82(10):2849.
[10] TamerEI-Raghy;Michel W;Barsoum;Antonios Zavaliangos et al.[J].Journal of the American Ceramic Society,1999,82(10):2855.
[11] N F Gao;Y Miyamoto;D Zhang.[J].Journal of Materials Science,1999(34):4358.
[12] C Racault;F Langhais;R Naslain.[J].ibid,1994(29):3384.
[13] Sun Zhimei;Zhang Yi;Zhou Yanchun .[J].Scripta Materialia,1999,1(01):61.
[14] R.Radhakrishnan;J.J.Williams .Synthesis and high-temperature stability of Ti3SiC2[J].Journal of Alloys and Compounds: An Interdisciplinary Journal of Materials Science and Solid-state Chemistry and Physics,1999(1/2):85-88.
[15] Jing-Feng Li;Fumiaki Sato;Ryuzo Watanabe.[J].Journal of Materials Science Letters,1999(18):1595.
[16] T Rudnik;J Lis.[J].ARCHIVES OF METALLURGY,1997(42):59.
[17] M W Barsoum;T EI-Raghy;L Ogbuji .[J].Journal of the Electrochemical Society,1997,144(07):2508.
[18] W Barsoum;T EI-Raghy;C Rawn;M W Barsoum.[J].Journal of Physics and Chemistry of Solids,1999(60):429.
[19] Alison Crssiey;Erich H Kisi;J W Bennett Summers.[J].Journal of Applied Physics,1999(32):632.
[20] Leonid Farber;Michel W .Barsoum Antonios Zavaliangos,Tamer EI-Raghy[J].Journal of the American Ceramic Society,1997,8(06):1677.
[21] C. J. Gilbert;D. R. Bloyer .FATIGUE-CRACK GROWTH AND FRACTURE PROPERTIES OF COARSE AND FINE-GRAINED Ti_3SiC_2[J].Scripta materialia,2000(8):761-767.
[22] T EI-Raghy;Antonios Zavaliangos;M W Barsoum et al.[J].Journal of the American Ceramic Society,1997,80(02):513.
[23] M.W. Barsoum;L. Farber;T. EI-Raghy.Dislocations Kink Bands, and Room-Temperature Plasticity of Ti3 SiC2[J].,1999(30A):1727-38.
[24] It Ment Low;Seung Knn Lee;Brian R;Lawn .[J].Journal of the American Ceramic Society,1998,81(01):225.
[25] 南策文;黄勇 .欧阳世翕[J].材料导报,2001,15(01):14.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%