对含钒微合金化钢连铸坯的高温塑性及变形试样中钒的碳、氮化物析出量进行了研究.研究结果表明,钒的碳、氮化物析出比在900~825 ℃之间最高,825 ℃时钒的碳、氮化物析出速率最大,在800~700 ℃之间,变形试样中仍有10 %~17 %钒的碳、氮化物析出.钒对钢在第Ⅲ脆性温度区的塑性有较大的影响,含钒高的钢铸坯试样脆化程度严重,且脆化向低温方向延伸.

参考文献

[1] Turkdogan E T.Causes and Effects of Nitride and Carbonitride Precipitation in HSLA Steels in Relation to Continuous Casting[A].,1987:70:399.
[2] Mintz B;Yue S;Jonas J J .Hot Ductility of Steels and Its Relationship to the Problem of Transverse Cracking During Continuous Casting[J].International Materials Reviews,1991,36:187.
[3] Kiichi Narita .Fundamental Study on Isolation and Determination of Carbide in Steels[J].Tetsu To Hagane-Journal of The Iron and Steel Institute of Japan,1980,66:2119.
[4] 王新华;昌波 .700~1000 ℃间含 Nb 钢铸坯的延塑性降低与Nb(C ,N)析出[J].金属学报,1997,33:485.
[5] 王新华;吴冬梅 .X-52管线钢连铸坯高温变形试样中碳、氮化物的析出和钢的高温延性[J].钢铁,1997,32(11):47.