Al-alloy (AA5022) corrosion penetration (CP) and crystal structure were investigated after running static immersion corrosion tests in 1 mol/L HCl solution and different concentrations of rare earth elements (La3+), (Ce3+) and their combination, at different temperatures. X-ray diffraction (XRD) was used to examine the surface structure before and after immersion, and secondary electron detector (SED) was operated to study surface morphology. In 1 mol/L HCl solution the corrosion penetration increased with increasing temperature and immersion time. The increase of La3+ concentrations up to 1000× 10-6 g/L led to the decrease in the corrosion penetration, and the decrease in Ce3+concentrations up to 50×10-6 g/L decreases the corrosion penetration of the alloy. Mix3 (combination of La3+ and Ce3+) dramatically reduced the corrosion penetration. This suggests that a synergistic effect exists between La3+and Ce3+. The reaction kinetics both in absence and presence of La3+ and Ce3+ and their combination would follow a parabolic rate law. The XRD patterns revealed that the intensities of certain hkl phases are affected. The crystalline structure has not been deformed either before or after testing and there are no additional peaks except that of the as-received alloy. In the case of accelerating CP, the surface morphology shows that the roughness andvoids of surface are increased.

参考文献

[1] R A Higgines.Engineering Metallurgy[M].The English Universities Press Ltd London,1965
[2] T R Beck .[J].Electrochimica Acta,1988,33:1321.
[3] L.Tomascanyi;K.Varga;J.Bartik;E.Maleczki .[J].Electrochimica Acta,1989,34:855.
[4] P.L.Cabot;F.A.Centellas;J.A.Gorrido;A.Perez H.Vidal .[J].Electrochimica Acta,1991,6:179.
[5] R Ambat;E S Dwarakodasa .[J].Journal of Applied Electrochemistry,1994,24:911.
[6] V.Branzoi;F.Golgovici;F.Branzoi .[J].Materials Chemistry and Physics,2002,78:122.
[7] F D Bogar;R T Foley .[J].Journal of the Electrochemical Society,1972,119:462.
[8] L.Tomcsany;K.Varga;I.Bartik;G.Horayni E.Maleczki .[J].Electrochimica Acta,1989,34:855.
[9] S E Frers;M M Stefenel;C.Mayer;T.Chierchie .[J].Journal of Applied Electrochemistry,1990,20:996.
[10] I L Rozenfeld.[M].Corrosion Inhibitors McGraw Hill New York,1981:182.
[11] M.N.Desai;B.C.Thakar;P.M.Chiaya;M.H.Gandi .[J].Corrosion Science,1976,16:9.
[12] S L Granse;B M Rosales .in Proc. 7th Eutopean Sym.on Corrosion Inhibitors, Ann[J].Univ Ferrara N S Sez V,1990,9:73.
[13] N Hackerman;H Kaesche .[J].Journal of the Electrochemical Society,1958,105:191.
[14] 陈绍杰.从第33届国际SAMPE年会看复合材料研究和应用的发展[J].材料工程,1989(01):11.
[15] R J Lash.in Proc. of the 6th Automotive Corrosion and Prevention Conf[M].Society of Automotive Engineers Warrendale PA,1993:153.
[16] N. Mora;E. Cano;J.L. Polo;J.M. Puente;J.M. Bastidas .Corrosion protection properties of cerium layers formed on tinplate[J].Corrosion Science,2004(3):563-578.
[17] B R W Hinton .[J].Metal Finishing,1991,89:55.
[18] A.E.Hughes;J.D.Gorman;P.J.K.Paterson .[J].Corrosion Science,1997,38:1957.
[19] S.M. Cohen .Review; Replacements for Chromium Pretreatments on Aluminum[J].Corrosion: The Journal of Science and Engineering,1995(1):71-78.
[20] B R W Hinton;N E Ryan;D R Anolt .[J].Materials Australia,1987,19:18.
[21] A B Brown .[J].Journal of the Electrochemical Society,1987,134(10):2506.
[22] L A Pawlick;R G Kelly .[J].Journal of Corros Sci Eng,1995,1:15.
[23] C.S.Brossia;E.Gileadi;R.G.Kelly .[J].Corrosion Science,1995,37(09):1455.
[24] M.Chiba;M.Seo .[J].Corrosion Science,2002,44:2378.
[25] M Chiba;M Seo .[J].Journal of the Electrochemical Society,2003,150(11):525.
[26] B Boubeker;J P Eymery;P Goudaeu;K.Bouslykkane J.P.Villian .[J].Annali di Chimica France,1994,19:377.
[27] M. Idiri;B. Boubeker;R. Sabot;Ph. Goudeau;J-F. Dinhut;J-L. Grosseau-Poussard .Structure and related corrosion behaviour in 1MH{sub}2SO{sub}4 of b.c.c.304l films prepared by ion beam sputtering[J].Surface & Coatings Technology,1999(2/3):230-234.
[28] P. Goudeau;J.L. Bechade;B. Boubeker;P.-O. Renault;A. Serrari;J.P. Eymery .X-ray diffraction analysis of texture modification induced by ion beam irradiation in stainless steel films[J].Applied Surface Science: A Journal Devoted to the Properties of Interfaces in Relation to the Synthesis and Behaviour of Materials,2004(1/4):151-157.
[29] A.J.Davenport;H.S.Isaacs;M.W.Kending .[J].Corrosion Science,1991,32:653.
[30] B R W Hinton;D R Anott;N E Ryan .[J].Materials Forum,1986,9:162.
[31] A.E.Hughes;R.J.Taylor;B.R.W.Hinton;L.Wilson .[J].Surface and Interface Analysis,1995,23:540.
[32] S Szklarska Smialowska .[J].Corrosion Science,1992,33:1193.
[33] E.J.Lee;S.I.Pyun .[J].Corrosion Science,1995,37(01):157.
[34] T H Nguyen;R T Foley .[J].Journal of the Electrochemical Society,1980,127:2563.
[35] N N Greenwood;A Earnshaw.Chemistry of the Elements, Pergamon Press[M].Oxford England,1984:243.
[36] S.Rajendran;S.Mary Reenkala;N.Anthony;R.Ramaraj .[J].Corrosion Science,2002,44:2243.
[37] R A Higgins.Engineering Metallurgy, Part Ⅰ[M].Applied Physical Metallurgy Ch. Ⅳ,1957:67.
[38] K.R.Trethewey;J.Chamerlain.Corrosion for Science and Engineering[M].Longman Group Ltd Essex England,1988:144.
[39] A K Cheetham;P Day.Solid State Chemistry[M].Oxford Science Publications,1987:42.
[40] B D Cullity.Elements of X-ray Diffraction, 2nd ed[M].Addison Wesley Publishing Company London,1987
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%