以Y_2O_3 和Nd_2O_3为原料,采用溶胶-凝胶燃烧法制备出Nd:Y_2O_3激光陶瓷纳米粉体.XRD测试结果表明粉体的最佳煅烧温度为1000 ℃,并且晶化完全.原子力显微镜观察结果表明粉体的粒度约为200 nm,分布均匀.差热-热重分析表明,柠檬酸在447 ℃分解放热, 而晶型转变温度为590 ℃,荧光光谱测试表明粉体最强的荧光发射峰位于9421.646 cm~(-1)(即波长1061.4 nm处) ,是 Nd~(3+4)F_(3/2)-~4I_(11/2)谱相导致的荧光发射.

The Nd:Y_2O_3 laser ceramic precusor was prepared by sol-gel combustion method, and Y_2O_3 and Nd_2O_3 were used as raw materials.XRD analysis showed that the optimum calcined temperature of precursor was 1000 ℃. At the same time crystallization was completed.The analysis of DTA-TG indicated that the citric acid was decomposed at 447 ℃,and the temperature of crystal inversion was 590 ℃.The strongest fluorescence peak of Nd:Y_2O_3 laser ceramics precursor was 9421.646 cm~(-1), that was Nd~(3+4)F_(3/2)-~4I_(11/2).

参考文献

[1] 刘颂豪.激光陶瓷--固体激光工作物质探索的新热点[J].激光与红外,2005(06):385-390.
[2] Ikesue A.;Kamata K.;Yoshida K.;Kinoshita T. .FABRICATION AND OPTICAL PROPERTIES OF HIGH-PERFORMANCE POLYCRYSTALLINE ND-YAG CERAMICS FOR SOLID-STATE LASERS[J].Journal of the American Ceramic Society,1995(4):1033-1040.
[3] Li Y;Zhu D C;Shen J et al.Synthesis of fine Y_2O_3:Eu phosphor by solid-state reaction at ambient temperature and its luminescent properties[J].Journal of Rare Earths,2006,26(zk):44-46.
[4] 霍地,张劲松,杨洪才,曹小明.用柠檬酸溶胶凝胶法合成SrFeCo0.5Ox氧化物[J].东北大学学报(自然科学版),2003(01):61-63.
[5] 王介强,郑少华,岳云龙,陶珍东,孙旭东.低温法制取Y2O3透明陶瓷的研究[J].无机材料学报,2003(06):1222-1228.
[6] 楼祺洪,马海霞,漆云凤,董景星,魏运荣.Yb3+:Y2O3透明陶瓷激光器获得5 W连续激光输出[J].光学学报,2004(03):431-432.
[7] 梅燕,聂祚仁,王为.利用红外光谱分析有机羧酸在均相反应中的配位作用机理[J].光谱学与光谱分析,2007(02):254-258.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%