采用动电位极化曲线和电化学阻抗谱结合光学显微镜研究了超级双相不锈钢SAF2507焊接接头经不同温度固溶处理后在高温浓磷酸中电化学行为.结果表明:2507不锈钢固溶处理可以改善原始焊接接头的组织提高其耐蚀性能;其中经950℃固溶处理后的焊接接头自腐蚀电流密度和致钝电流密度较小,极化后的电极表面点蚀较轻;腐蚀行为受电荷转移电阻和有限扩散层的混合控制,符合半无限扩散过程的特征;经950℃固溶处理后焊接接头在高温浓磷酸中形成的钝化膜较为致密.

Electrochemical behavior of stainless steel SAF2507 weld joints after solution treatment in high-temperature concentrated phosphoric acid solution was investigated by means of polarization curve,electrochemical impedance spectroscopy and optical microscope.The results show that solution treatment can improve the microstructure of the welding joint and then improve its corrosion resistance.After solution treatment at 950 ℃,the welding joint shows the smaller corrosion current and critical passive current density,and its electrode surface has the lighter pitting after polarization.The corrosion process belongs to the mixed control of charge transfer resistance and Warburg resistance,and comply with the characteristics of semi-infinite diffusion process.The passivation film of the welding joint in hightemperature concentrated phosphoric acid is the densest after solution treatment at 950 ℃.

参考文献

[1] CHWEE-SIM GOH;TICK-HON YIP.Fatigue Deformation-Induced Response in a Superduplex Stainless Steel[J].Metallurgical and Materials Transactions, A. Physical Metallurgy and Materials Science,200211(11):3433-3442.
[2] F. Kolenic;L. Kovac;D. Drimal.Effect of LASER welding conditions on AUSTENITE/FERRITE RATIO in DUPLEX STAINLESS STEEL 2507 welds[J].Welding in the World: Journal of the International Institute of Welding: Journal of the International Institute of Welding,20115/6(5/6):19-25.
[3] Sato YS;Nelson TW;Sterling CJ;Steel RJ;Pettersson CO.Microstructure and mechanical properties of friction stir welded SAF 2507 super duplex stainless steel[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,20051/2(1/2):376-384.
[4] 谭华 .双相不锈钢焊缝组织演变与腐蚀行为研究[D].复旦大学,2012.
[5] 龚利华;张波;王赛虎.超级双相不锈钢焊接接头的耐蚀性能[J].焊接学报,2010(7):59-62.
[6] 龚利华;张欢;程东亮.保护气体氮对双相不锈钢焊接接头腐蚀行为的影响[J].材料热处理学报,2013(9):112-115.
[7] 刘焕安;叶际宣.湿法磷酸工业中不锈钢应用综述[J].腐蚀科学与防护技术,2012(04):267-274.
[8] C. S. Frankel;N. Sridhar.Understanding localized corrosion[J].Materials Today,200810(10):38-44.
[9] 李涛;李晓刚;董超芳;周建龙;冯佃臣;吴军.Cl~-含量对2A12铝合金初期腐蚀行为的影响[J].北京科技大学学报,2009(12):1576-1582.
[10] Jean-Baptiste Jorcin;Mark E. Orazem;Nadine Pebere;Bernard Tribollet.CPE analysis by local electrochemical impedance spectroscopy[J].Electrochimica Acta,20068/9(8/9):1473-1479.
[11] A. J. RAMIREZ;J. C. LIPPOLD;S. D. BRANDI.The Relationship between Chromium Nitride and Secondary Austenite Precipitation in Duplex Stainless Steels[J].Metallurgical and Materials Transactions, A. Physical Metallurgy and Materials Science,20038(8):1575-1597.
[12] Henrik Sleurin;Rolf Sandstrom.Austenite reformation In the heat-affected zone of duplex stainless steel 2205[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,20061/2(1/2):250-256.
[13] Badji, R;Bouabdallah, M;Bacroix, B;Kahloun, C;Bettahar, K;Kherrouba, N.Effect of solution treatment temperature on the precipitation kinetic of sigma-phase in 2205 duplex stainless steel welds[J].Materials Science and Engineering. A, Structural Materials: Properties, Microstructure and Processing,20081/2(1/2):447-454.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%