采用粉末冶金法制备烧结Sm(Co0.72Fe0.15Cu0.1Zr0.03)7.5,研究磁粉粒度对磁体磁性能的影响.结果表明,增加球磨时间将细化磁粉粒度,提高磁粉的比表面积,有利于降低磁体的烧结温度.球磨5,7,9,11 h的磁粉的最佳烧结温度分别为1225,1225,1215,1215 ℃.磁粉球磨9 h,烧结温度为1215 ℃条件下制备的磁体的综合磁性能最优:剩磁Br=0.94 T,感应矫顽力Hcb=708.4 kA·m-1,最大磁能积(BH)max=171.9 kJ·m-3,内禀矫顽力Hci=2276.6 kA·m-1;温度稳定性良好,长径比为0.7的磁体经550 ℃老化2 h后的磁通不可逆损失低于5%,有望应用于550 ℃环境中.

参考文献

[1] Ojima T;Tomizawa S;Yoneyama T et al.Magnetic properties of a new type of rare earth cobalt magnets[J].IEEE Transactions on Magnetics,1977,13(05):1317.
[2] Ray A E .The development of high energy product permanent magnets from 2:17 RE-TM alloys[J].IEEE Transactions on Magnetics,1984,20(05):1514.
[3] Kim AS. .DESIGN OF HIGH TEMPERATURE PERMANENT MAGNETS[J].Journal of Applied Physics,1997(8 Pt.2b):5609-5611.
[4] Ma B.M.;Liang Y.L. .The effect of Fe on the temperature dependent magnetic properties of Sm(Co,Fe,Cu,Zr)/sub z/ and SmCo/sub 5/ sintered magnets at 450/spl deg/C[J].IEEE Transactions on Magnetics,1996(5):4377-4379.
[5] Liu S.;Hoffman E.P. .Application-oriented characterization of Sm/sub 2/(Co,Fe,Cu,Zr)/sub 17/ permanent magnets[J].IEEE Transactions on Magnetics,1996(5):5091-5093.
[6] Chen CH.;Walmer MH.;Liu S.;Kuhl E.;Simon G.;Walmer MS. .Sm-2(Co,Fe,Cu,Zr)(17) magnets for use at temperature >= 400 degrees C[J].Journal of Applied Physics,1998(11 Pt.2):6706-6708.
[7] Liu J.F.;Ding Y.;Hadjipanayis G.C. .Effect of iron on the high temperature magnetic properties and microstructure of Sm(Co, Fe, Cu, Zr)_z permanent magnets[J].Journal of Applied Physics,1999(3):1670-0.
[8] Tang W;Zhang Y;Hadjipanayis G C .Microstructrue and magnetic peoperties of Sm(CobalFexCu0.128Zr0.02)7.0 magnets with Fe substitution[J].Journal of Magnetism and Magnetic Materials,2000,221:268.
[9] 李春和,戴雨兰,龙毅,强文江.新型钐钴永磁的高温性能和微观结构[J].中国稀土学报,2002(z2):80-82.
[10] 杜娟,易健宏,彭元东,李丽娅,罗述东,唐新文.2∶17 型SmCo永磁材料的研究进展与展望[J].中国稀土学报,2002(z2):76-79.
[11] 周寿增.稀土永磁材料及其应用[M].北京:冶金工业出版社,1995:180.
[12] Nagel H .Coercivity and microstructure of Sm(Co0.87Cu0.13)7.8[J].Journal of Applied Physics,1979,50(02):1026.
[13] Scholz W.;Fidler J.;Schrefl T.;Suess D.;Matthias T. .Micromagnetic three-dimensional simulation of the pinning field in high temperature Sm(Co,Fe,Cu,Zr)(z) magnets[J].Journal of Applied Physics,2002(10 Pt.3):8492-8494.
[14] Rong C B;Zhang H W;Jian J et al.Microstructure simulation of the coercivity mechanism in Sm(Co,Fe,Cu,Zr)z magnets[J].Journal of Applied Physics,2004,95(03):1351.
[15] Cataldo L;Lefèvre A;Ducret F et al.Binary system Sm-Co:Revision of the phase diagram in the Co-rich field[J].Journal of Alloys and Compounds,1996,241:216.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%