采用三点弯曲法测定了SiC纤维单向增强的Ti-6Al-4V复合材料的表观断裂韧性,讨论了界面反应对断裂韧性的影响.研究结果表明,在裂纹尖端塑性变形区的未断纤维的桥联对复合材料的断裂韧性起很大的作用.经过热处理后,SiCf/Ti-6Al-4V复合材料的断裂韧性降低,主要是由于严重的界面反应,使得SiC纤维受到一定的损伤,因而降低了纤维的承载能力,并使基体钛合金的脆性增大.

Apparent fracture toughness of the Ti-6Al-4V alloy uniaxiaUy reinforced with SiC fibers was measured by three-point bending test and the effect of the interfacial reaction on toughness was discussed.It is pointed out that bridging of the intact fibers in plastic zone ahead of the crack tip plays an important role for fracture toughness of the composites.And fracture toughness of the heat-treated composites decreases due to the severe interfacial reaction that leads to damage of the SiC fibers and therefore the decrease of the load-beating ability,and to the increase of the brittleness in the titanium matrix.

参考文献

[1] Carlos Gonzalez;Javier LLorca;Arnaud Week .Toughness of fiber-reinforced titanium as a function of temperature: experimental results and micromechanical modeling[J].Acta materialia,2004(13):3929-3939.
[2] 杨延清,马志军,吕祥鸿,李健康,陈彦,艾云龙.SiCf/Ti-6Al-4V复合材料的界面研究[J].稀有金属材料与工程,2006(10):1516-1521.
[3] Yang Y Q;Ma Z J;Lü X H et al.Microstructure and micromechanics of the interface of SiCf/Ti-6Al-4V composites[J].Rare Metal Materlals and Engineering,2006,35(Supp 1):301-304.
[4] Y. Q. Yang;Y. Zhu;Z. J. Ma .Formation of interfacial reaction products in SCS-6 SiC/Ti_2AlNb composites[J].Scripta materialia,2004(5):385-389.
[5] Y.Q. Yang;H.J. Dudek;J. Kumpfert .MICROSTRUCTURE OF INTERFACIAL REGION OF SCS-6 SiC/TiB_2/Ti_2AlNb COMPOSITE[J].Scripta materialia,2001(11):2531-2536.
[6] Yang Y Q;Zhu Y;Ma Z J.Intedacial reaction of super α2 and Ti2 AlNb composites reinforced by SCS-6 SiC fibers[A].Weinheim:Wiley-VCH Verlag,2004:2479-2486.
[7] Li J K;Yang Y Q;Yuan M N et al.The effect of properties of SiC fiber on longitudinal tensile behavior of SiC/Ti-6Al-4V composites[J].Transactions of Nonferrous Metals Society of China,2008,18(03):523-530.
[8] 李建康,杨延清,罗贤,张荣军.SiC纤维增强钛基复合材料的横向力学性能[J].稀有金属材料与工程,2009(03):426-430.
[9] Kamat S V;Hirth J P;Zok F W .Effect of notch root radius on crack initiation and growth toughness of A cross-ply Ti-6Al-4V/SiC composite[J].Acta Materialia,1996,44(05):1831-1838.
[10] Thouless D B;Evans A G .Effects of pull-out on the mechanical properties of ceramic matrix composites[J].Acta Materialia,1988,36(03):517-522.