采用L9(34)正交实验方法,研究了弹性体乙烯-辛烯共聚物(8003树脂)、增容剂乙烯-丙烯酸共聚物(EAA)、滑石粉及增塑剂甘油对淀粉/乙烯-醋酸乙烯酯(EVA)复合发泡鞋底材料力学性能的影响,并通过X射线衍射(XRD)和扫描电镜(SEM)表征了共混物的结构.结果表明,滑石粉和8003树脂对共混物的拉伸强度、延伸率及回弹性有显著的影响,当8003树脂为20phr、EAA为30phr、滑石粉为0phr、甘油为8phr时,共混物的综合力学性能最好.XRD和SEM分析表明,EAA的加入能大大增加淀粉和EVA的相容性,达到增容的效果.

参考文献

[1] Qi B;Yue Z .Fluorescence from an azobenzene-containing diblock copolymer micelle in solution[J].Langmuir: The ACS Journal of Surfaces and Colloids,2007(10):5746-5751.
[2] Abraham Ulman .Formation and Structure of Self-Assembled Monolayers[J].Chemical Reviews,1996(4):1533-1554.
[3] Suprakas Sinha Ray;Mosto Bousmina .Biodegradable polymers and their layered silicate nanocomposites: In greening the 21st century materials world[J].Progress in materials science,2005(8):962-1079.
[4] 刘现峰,王苓.淀粉的塑化研究进展[J].山东化工,2007(02):38-40.
[5] Pandey, JK;Reddy, KR;Kumar, AP;Singh, RP .An overview on the degradability of polymer nanocomposites[J].Polymer Degradation and Stability,2005(2):234-250.
[6] 梅超群,张洪利.淀粉塑料发展现状及其前景展望[J].化工时刊,2007(01):63-65.
[7] 钱志国,王永涛,韩宇,任天斌.改性淀粉/EVA共混低成本热熔胶的制备及性能研究[J].中国胶粘剂,2009(07):17-21.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%