以碳酸锂、氧化钴为主要原料,掺入化学计量的超细二氧化锆、超细二氧化钛,按球料比3:1,在转速500r/min经1h行星式球磨后,经900℃固相烧结制备了锂离子电池正极材料LiCo0.9Zr0.03Ti0.07O2,用X射线衍射(XRD)、扫描电镜(SEM)对材料的结构与形貌进行了研究,结果表明Li0.9Zr0.03Ti0.07O2与LiCoO2一样具有六方层状结构.在0.2C倍率下材料的初始放电容量达147mAh/g,2C倍率下初始放电容量达140.5mAh/g,3.6V放电平台比例达89.6%,500次循环后容量衰减7.5%,材料大电流放电性能好、循环寿命长.
参考文献
[1] | Huang B;Jang Y I;Chiang Y M et al.[J].Journal of Applied Electrochemistry,1998,28:1365. |
[2] | Liu Y;Fujiwara T;Yukawa H et al.[J].E1ectrochimica Acta,2001,46:1151. |
[3] | Cubo K;Fujiwara M;Yamada S et al.[J].Journal of Power Sources,1997,68:553. |
[4] | Kalaiselvi N;Doh CH;Park CW;Moon SI;Yun MS .A novel approach to exploit LiFePO4 compound as an ambient temperature high capacity anode material for rechargeable lithium batteries[J].Electrochemistry communications,2004(11):1110-1113. |
[5] | Patoux S;Doeff M M .[J].Electrochemistry Communications,2004,6:767. |
[6] | 郝万君,陈岗,史延慧.Al掺杂对Li(AlyCo1-y)O2材料结构的影响[J].高等学校化学学报,2001(02):175-178. |
[7] | Myung ST.;Komaba S.;Chung HT.;Kumagai N. .Effects of Al doping on the microstructure of LiCoO2 cathode materials[J].Solid state ionics,2001(1/2):47-56. |
[8] | 杨箫,倪江锋,黄友元,陈继涛,周恒辉,张新祥.钛掺杂对不同形貌LiCoO2电化学性能的影响[J].物理化学学报,2006(02):183-188. |
[9] | Han CH.;Hong YS.;Kim K. .Cyclic performances of HT-LiCo0.8M0.2O2 (M=Al, Ni) powders prepared by the molten salt synthesis method[J].Solid state ionics,2003(3/4):241-247. |
[10] | Zhao Hailei;Gao Ling;Qiu Weihua et al.[J].Journal of Power Sources,2004,132:195. |
[11] | Madhavi S;Rao G V;Chowdari B V R et al.[J].Electrochimica Acta,2002,48:219. |
[12] | Aurbach D;Markovsky B;Rodkin A et al.[J].Electrochimica Acta,2002,47:4291. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%