ERH end-quenching method was us ed to determine the hardenability of four kinds hot-forging die steels with dee p-hardening and hence the order of their hardenability was given. The tempering hardness of the steels was measured and the tempering resistance was studied. It was approved that ERH method is effective for the determination of hardenability of deep-hardening steel and the beginning of hardness drop in the ERH specimen is caused by bainite occurring.

参考文献

[1] Hao S M;Zong Y P;Zhang B R et al.A Study on the Method for Measuring Hardenability of High Hardenability Steels[J].J Anhui Insti Tech(in Chinese),1988,7(02):251-256.
[2] Zong Y P;Hao S M;Zhang B R et al.Effect of Adjusting Alloying Elements on Hardenability of Steel 5CrNiMo[J].Journal of Northeast Univ Tech(in Chinese),1991,12(04):356-360.
[3] Siebert C A;Doane D V;Breen D H.The Hardenability of Steels[M].American Society for Metals.Ohio:Metals Park,1977
[4] Pickering F B.Vanadium as a Hardenability and Temperability Add itive in Quenched and Tempered Steels[A].Beijing:ASM,1985:305-324.
[5] Mangonon P L .The Heat Treatment of Vanadium-Modified Alloy Steels[J].Journal of Metals,1981,33(06):18-24.
[6] Grang R A;Hribal C R;Porter L F .Hardness of Tempered Martensite in Carbon and Low-Alloy Steels[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,1977,8(11):1775-1785.
[7] Jiang Z G;Chen Z Z;Ren M E.Die Steel[M].北京:冶金工业出版社,1988