低水胶比的混凝土在水化过程中会有较大的化学收缩和自干燥,从而导致在硬化过程中产生较高的自收缩变形.混凝土的自收缩变形被限制内部就会产生拉应力,拉应力超过混凝土抗拉强度,最终就会产生裂缝.这些裂缝严重影响混凝土结构的耐久性.为了减少混凝土的化学收缩和自收缩,高吸水树脂作为内养护剂掺加到混凝土中.通过论述国内外高吸水树脂作为混凝土内养护剂的研究进展,对高吸水树脂在混凝土应用的发展前景进行了展望.

参考文献

[1] Daniel Cusson;Ted Hoogeveen .Internal curing of high-performance concrete with pre-soaked fine lightweight aggregate for prevention of autogenous shrinkage cracking[J].Cement and Concrete Research,2008(6):757-765.
[2] Igor De la Varga;Javier Castro;Dale Bentz .Application of internal curing for mixtures containing high volumes of fly ash[J].Cement & concrete composites,2012(9):1001-1008.
[3] Arnon Bentur;Shin-ichi Igarashi;Konstantin Kovler .Prevention of autogenous shrinkage in high-strength concrete by internal curing using wet lightweight aggregates[J].Cement and Concrete Research,2001(11):1587-1591.
[4] D. Snoeck;S. Steuperaert;K. Van Tittelboom .Visualization of water penetration in cementitious materials with superabsorbent polymers by means of neutron radiography[J].Cement and Concrete Research,2012(8):1113-1121.
[5] Esteves, L.P. .On the hydration of water-entrained cement-silica systems: Combined SEM, XRD and thermal analysis in cement pastes[J].Thermochimica Acta: An International Journal Concerned with the Broader Aspects of Thermochemistry and Its Applications to Chemical Problems,2011(1/2):27-35.
[6] Christof Schrofl;Viktor Mechtcherine;Michaela Gorges .Relation between the molecular structure and the efficiency of superabsorbent polymers (SAP) as concrete admixture to mitigate autogenous shrinkage[J].Cement and Concrete Research,2012(6):865-873.
[7] 李铁军 .自养护高性能混凝土抗侵蚀及收缩试验研究[D].宁夏大学,2011.
[8] Yan Yao;Yu Zhu;Yingzi Yang .Incorporation superabsorbent polymer (SAP) particles as controlling pre-existing flaws to improve the performance of engineered cementitious composites (ECC)[J].Construction and Building Materials,2012(1):139-145.
[9] 何真,陈衍,梁文泉,杨华全.内养护对混凝土收缩开裂性能的影响[J].新型建筑材料,2008(08):7-11.
[10] 孙婧,元敬顺,刘宏波,白润山,丛晓红.不同龄期的高流态自养护泵送混凝土性能的试验研究[J].硅酸盐通报,2013(04):623-629.
[11] Ali Pourjavadi;Seyed Mahmoud Fakoorpoor;Alireza Khaloo;Payam Hosseini .Improving the performance of cement-based composites containing superabsorbent polymers by utilization of nano-SiO_2 particles[J].Materials & design,2012(Dec.):94-101.
[12] Ali Pourjavadi;Seyed Mahmoud Fakoorpoor;Payam Hosseini.Interactions between superabsorbent polymers and cement-based composites incorporating colloidal silica nanoparticles[J].Cement & concrete composites,2013:196-204.
[13] A.M. Soliman;M.L. Nehdi .Effect of partially hydrated cementitious materials and superabsorbent polymer on early-age shrinkage of UHPC[J].Construction and Building Materials,2013(Apr.):270-275.
[14] 丁以兵,詹炳根,黄其海,周万良.自养护作用下的高性能混凝土抗冻与抗渗性能[J].合肥工业大学学报(自然科学版),2007(05):603-606.
[15] 陈德鹏,钱春香,高桂波,赵洪凯.高吸水树脂对混凝土收缩开裂的改善作用及其机理[J].功能材料,2007(03):475-478.
[16] 陈德鹏,钱春香,赵洪凯,高桂波.内养护措施改善混凝土收缩开裂性能[J].特种结构,2007(01):57-60.
[17] 姚明甫,詹炳根.养护对高性能混凝土塑性收缩的影响[J].合肥工业大学学报(自然科学版),2005(02):180-184.