研究了N36锆合金包壳管在温度为593~723 K、应力为60~160MPa条件下的拉伸蠕变行为.结果表明,本试验条件下N36锆合金管材存在不同的蠕变变形机制.593~673K下低应力范围内,蠕变应力因子n约为3,蠕变表观激活能Qapp≈150 kJ·mol-1,蠕变变形受位错的粘滞性滑移过程控制;高应力范围内蠕变应力因子n为5~6,蠕变激活能Qapp≈170 kJ·mo1-1,遵循典型的5次幂律蠕变规律,蠕变变形受位错攀移过程控制.在723 K时,高应力范围内发生幂律失效.N36锆合金包壳管表现为典型的ClassA型合金蠕变特征,表现出与Zircaloy合金不同的蠕变规律.

参考文献

[1] Moon JH;Cantonwine PE;Anderson KR;Karthikeyan S;Mills MJ .Characterization and modeling of creep mechanisms in Zircaloy-4[J].Journal of Nuclear Materials: Materials Aspects of Fission and Fusion,2006(3):177-189.
[2] Nam C.;Choi BK.;Lee MH.;Jeong YH. .Creep strength of Zircaloy-4 cladding depending on applied stress and annealing temperature[J].Journal of Nuclear Materials: Materials Aspects of Fission and Fusion,2002(1):70-76.
[3] Charit I;Murty KL .Creep behavior of niobium-modified zirconium alloys[J].Journal of Nuclear Materials: Materials Aspects of Fission and Fusion,2008(3):354-363.
[4] 赵文金,周邦新,苗志,彭倩,蒋有荣,蒋宏曼,庞华.我国高性能锆合金的发展[J].原子能科学技术,2005(z1):2-9.
[5] 彭继华,李文芳,Jean-Luc Bechade,R.Maury.织构对先进锆合金蠕变性能各向异性的影响[J].稀有金属,2008(01):1-6.
[6] 赵文金.核工业用高性能锆合金的研究[J].稀有金属快报,2004(05):15-20.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%