综述了当前常用的几种火电厂高温压力管道寿命预测的方法及模型,包括持久强度法、时间参数外推法、θ法与修正的。法、蠕变曲线外推法和蠕变损伤法,深入讨论了各方法适用条件和可靠性。最后,对与高温压力管道寿命预测有关的几个技术问题进行了分析和展望。

Several current life prediction methods and models for high temperature pressure pipes in thermal power plants were introduced, including persistent strength method time parameter exptrapolation method, 0 method and 0 method of amendment, gradual extrapolation method based on creep curves and creep damage method. The reliability of these methods was deeply discussed. Then application conditions and brief commentaries to these methods were given. Finally, several technical problems about life prediction of the high temperature pressure pipes were analyzed and predicted.

参考文献

[1] 束国刚,李益民,赵彦芬,梁昌乾,王荣山,陈国良,郭宏,孙继跃.基于蠕变曲线的12Cr1MoV钢寿命外推计算方法[J].热力发电,2000(06):32-35.
[2] 牛小驰,巩建鸣,姜勇,耿鲁阳,涂善东.基于损伤力学的电厂主蒸汽管道蠕变损伤有限元分析[J].中国电机工程学报,2008(20):32-37.
[3] A. A. Becker;T. H. Hyde;W. Sun;P. Andersson .Benchmarks for finite element analysis of creep continuum damage mechanics[J].Computational Materials Science,2002(1/2):34-41.
[4] 耿鲁阳,刘建杰,巩建鸣,姜勇,尹基奉,沈利民.基于修正θ投影法的炉管用Cr25Ni35Nb钢蠕变寿命预测[J].机械工程材料,2011(12):93-96.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%