高级检索

由于ZrB2具有极高的熔点、强度、硬度和导电率等许多优异性能,因而其应用领域非常广泛.研究了ZrB2-Si3N4复相陶瓷的制备和高温下的氧化机理.结果表明,在1700℃、15MPa、2h烧结务件下制备的ZrB2-20%Si3N4复相陶瓷的致密度为98%左右.ZrB2-Si3N4复相陶瓷在高温氧化时生成了SiO2,并且SiO2液相容易在复相陶瓷表面富集形成一层保护膜,有望提高陶瓷在更高氧化温度下的抗氧化性能.

参考文献

[1] Zhang X H;Li X Y;Han J C .Effects of Y2O3 on microstructure and mechanical properties of ZrB2-SiC ceramics[J].Journal of Alloys and Compounds,2008,465:506.
[2] Chamberlain A L;Fahrenholtz W G;Hilmal G E .Pressureless sintering of zirconium diboride[J].Journal of the American Ceramic Society,2006,89:450.
[3] Monteverde F .Ultra-high temperature UfB2-SiC ceramics consolidated by hot-pressing and spark plasma sintering[J].Journal of Alloys and Compounds,2007,428:197.
[4] Monteverde F.;Guicciardi S.;Bellosi A. .Advances in microstructure and mechanical properties of zirconium diboride based ceramics[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2003(1/2):310-319.
[5] Guo S;Hirosaki N;Yamamoto Y .Hot-pressed SigN4 ceramics with Lu2O3 additives:Grain-boundary phase and strength[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,2005,408:9.
[6] Houjou K;Ando K;Chu M C .Effect of sintering additives on the oxidatio behavior of Si3N4 ceramics at 1300℃[J].Journal of the European Ceramic Society,2005,25:559.
[7] F. EBLAGON;B. EHRLE;T. GRAULE .Development of silicon nitride/silicon carbide composites for wood-cutting tools[J].Journal of the European Ceramic Society,2007(1):419-428.
[8] Yamamoto H;Akiyama K;Murakami Y .Densification behaviors and high-temperature characteristics of SigN4 sintered bodies using Al2O3-Yb2O3 additives[J].Journal of the European Ceramic Society,2006,26:1059.
[9] Bernal M H B;Matovic B .Dense and near-net-shape fabrication of SisN4 ceramics[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,2009,500:130.
[10] Xu X;Mei S;Ferreira J .Fabrication of Si3N4-SiC nanocomposite ceramics through temperature-induced gelation and liquid phase sintering[J].Journal of the European Ceramic Society,2006,26:337.
[11] Kim H D;Park Y J;Han B D .Fabrication of dense bulk nano-Si3N4 ceramics without secondary crystalline phase[J].Scripta Materialia,2006,54:615.
[12] Diletta Sciti;Mylene Brach;Alida Beliosi .Oxidation behavior of a pressureless sintered ZrB_2-MoSi_2 ceramic composite[J].Journal of Materials Research,2005(4):922-930.
[13] Rezaie A;Fahrenholtz W G;Hilmas G E .Oxidation of zirconium diboride-silicon carbide at 1500℃ at a low partial pressure of oxygen[J].Journal of the American Ceramic Society,2006,89:3240.
上一张 下一张