Some of the major manufacturing processes and corresponding mechanical properties of titanium clad steel plates were analyzed, and the consequences of research, manufacturing, and application of titanium clad steel plates in both markets of China and overseas were also summarized. As an economical and environmentally friendly technology, the roll bonding process is ex-pected to become the next-generation mainstream process for the manufacturing of titanium clad steel plate. Some of the crucial and most important technical problems of this particular process, including vacuum sealing technology, surface treatment process technology, application of a transition layer, and rolling process, were discussed along with the advantageous mechanical properties and life-cycle economy of these plates processed by this technology. Finally, the market needs, application trends, and requirements of titanium clad steel plate were also considered from industries of petrochemical, shipbuilding, marine, and electric power.

参考文献

[1] L.Yan .[J].China Titanium Industry,2011,3:12-14.
[2] H.Y.Shi;J.X.Wang .[J].Building Construction,2005,27(4):65-66.
[3] T.Nakayama;A.Nagai;A.Yahiro .[J].Sumimoto Metal,1997,49:95-97.
[4] J.Song;A.Kostka;M.Veehmayer .[J].MATERIALS SCIENCE & ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING,2011,528:2641-2644.
[5] J.Z.Wang;X.B.Yan;W.Q.Wang .[J].Mater Rev,2005,19(4):61-63.
[6] T.Fukuda .[J].Bull Jpn Inst Met,1992,31:194-198.
[7] T.Fukuda;S.Yoshinori .[J].Tetsu-to-Hagane,1989,75:1162-1165.
[8] K.Bhanumurthy;G.B.Kale .[J].Journal of Materials Science Letters,1993,12:1879-1882.
[9] M.Ghosh;K.Bhanumurthy;G.B.Kale .[J].ISIJ International,2004,44:389-392.
[10] J.X.Liu;A.M.Zhao;H.T.Jiang .[J].Int J Miner Metall Mater,2012,19:404-408.
[11] H.T.Jiang;X.Q.Yan;J.X.Liu .[J].Transactions of Nonferrous Metals Society of China,2014,24:697-704.
[12] J.Z.Wang;X.B.Yan;W.Q.Wang .[J].Rare Metal Mater Eng,2010,39:309-312.
[13] E.Atasoy;N.Kahraman .[J].Materials Characterization,2008,59:1481-1485.
[14] S.Sam;S.Kundu;S.Chatterjee .[J].Mater Des,2012,40:237-244.
[15] S.Kundu;D.Roy;S.Chatterjee .[J].Mater Des,2012,37:560-568.
[16] S.Kundu;S.Sam;S.Chaterjee .[J].MATERIALS SCIENCE & ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING,2013,560:288-295.
[17] S.Nishida;T.Matsuoka;T.Wada .[J].JFE Tech Rep,2005,5:1-5.
[18] X.B.Wang;R.S.Liu;F.J.Fan .[J].Metal World,2010,1:53-56.
[19] S.Yoshiwara;T.Kawanami;K.Suzuki .[J].Tetsu-to-Hagane,1986,72:671-675.
[20] F.Kurosawa .[J].Surface and Interface Analysis,1988,12:203-206.
[21] S.Y.Jiang;S.C.Li .[J].Rare Metal Mater Eng,2011,40:38-42.
[22] Y.Ma;Y.Rong;J.Z.Wang .[J].Titanium Industry Progress,2010,27(2):24-27.
[23] X.W.Zhang;L.Li .[J].Steel Rolling,2013,30(6):45-49.
[24] J.Z.Wang;X.B.Yan .[J].Metal Heat Treatment,2009,2:81-84.
[25] C.J.Huang .[J].Rare Metals Letters,2002,6(3):34-38.
[26] J.Billingham;J.V.Sharp;J.Spurrier.Review of the Performance of High Strength Steels Used Offshore[M].Health & Safety Executive,Bedfordshire,2003
[27] K.Yoshihiko;K.Hiroyuki .[J].Kobelco Tech Rev,2013,63(32):1-8.
[28] W.Dai;X.A.Wu .[J].China New Technologies and Products,2012,3:1-2.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%