高级检索

用恒电流沉积方法分别在ZrO(NO3)2电解液和由Ca(NO3)2及NH4H2PO4组成的电解液中制备出羟基磷灰石/二氧化锆(HA/ZrO2)梯度医用复合涂层.通过扫描电镜观察,研究了沉积电流和沉积时间对涂层形貌的影响.结果表明,当沉积电流为11.1 mA,沉积时间为400 s时,在锆电解液中可获得均匀的钛基Zr(OH)4涂层;当沉积电流为1.1 mA,沉积时间为900 s时,含Zr(OH)4涂层的钛基在钙的磷酸盐电解液中得到了均匀致密的Zr(OH)4/HA复合涂层.该复合涂层经650℃热处理后形成HA/ZrO2梯度复合涂层.拉伸试验表明,HA/ZrO2复合涂层的结合强度从单一HA涂层的5MPa增加到17MPa以上.

参考文献

[1] Samar J. Kalita;Abhilasha Bhardwaj;Himesh A. Bhatt .Nanocrystalline calcium phosphate ceramics in biomedical engineering[J].Materials science & engineering, C. Biomimetic and supramolecular systems,2007(3):441-449.
[2] Suchanek W.;Yoshimura M. .Processing and properties of hydroxyapatite-based biomaterials for use as hard tissue replacement implants [Review][J].Journal of Materials Research,1998(1):94-117.
[3] 王周成,黄龙门.金属基生物活性羟基磷灰石涂层材料的研究进展[J].硅酸盐通报,2006(01):57-62,108.
[4] Lynn AK;DuQuesnay DL .Hydroxyapatite-coated Ti-6Al-4V part 1: the effect of coating thickness on mechanical fatigue behaviour.[J].Biomaterials,2002(9):1937-1946.
[5] Yang Y;Kim KH;Ong JL .A review on calcium phosphate coatings produced using a sputtering process-an alternative to plasma spraying.[J].Biomaterials,2005(3):327-337.
[6] R. Roop Kumar;M. Wang .Functionally graded bioactive coatings of hydroxyapatite/titanium oxide composite system[J].Materials Letters,2002(3):133-137.
[7] 熊信柏,李贺军,黄剑锋,李镇江,付业伟.医用碳材料对骨组织的响应及其生物活化改性[J].稀有金属材料与工程,2005(04):515-520.
[8] Piconi C;Maccauro G .Zirconia as a ceramic biomaterial.[J].Biomaterials,1999(1):1-25.
[9] Bang-Yen Chou;Edward Chang .Influence of deposition temperature on mechanical properties of plasma-sprayed hydroxyapatite coating on titanium alloy with ZrO{sub}2 intermediate layer[J].Journal of Thermal Spray Technology,2003(2):199-207.
[10] Khalil Abdelrazek Khalil;Sug Won Kim;Hak Yong Kim .Consolidation and mechanical properties of nanostructured hydroxyapatite-(ZrO_2 + 3 mol% Y_2O_3) bioceramics by high-frequency induction heat sintering[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2007(1/2):368-372.
[11] Chevalier JJ;Deville S;Munch E;Jullian R;Lair F .Critical effect of cubic phase on aging in 3mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis.[J].Biomaterials,2004(24):5539-5545.
[12] Inuzuka M;Nakamura S;Kishi S;Yoshida K;Hashimoto K;Toda Y;Yamashita K .Hydroxyapatite-doped zirconia for preparation of biomedical composites ceramics[J].Solid state ionics,2004(1/4):509-513.
[13] Yun-Mo Sung;Dae-Hee Kim .Crystallization characteristics of yttria-stabilized zirconia hydroxyapatite composite nanopowder[J].Journal of Crystal Growth,2003(3/4):411-417.
[14] YOSHIDA K;HASHIMOTO K;TODA Y et al.Fabrication of structurecontrolled hydroxyapatite/zirconia composite[J].Journal of the European Ceramic Society,2006,26(4/5):515-518.
[15] 王英波,鲁雄,赵婧,冯波,汪建新,屈树新,翁杰,陈建敏.脉冲电化学沉积制备n-HA/ZrO2复合涂层[J].稀有金属材料与工程,2009(06):1071-1075.
[16] 王英波,鲁雄,冯波,屈树新,翁杰.脉冲电沉积制备HA/ZrO_2纳米复合涂层的稳定性及生物相容性评价[J].高等学校化学学报,2010(02):253-259.
[17] AFSHAR A;GHORBANI M;EHSANI N et al.Some important factors in the wet precipitation process of hydroxyapatite[J].Materials & Design,2003,24(03):197-202.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%