对比研究了V-N微合金钢、C70S6BY两种汽车发动机裂解连杆用钢的疲劳强度、疲劳断口形貌和疲劳裂纹形成机理.结果表明,V-N微合金钢的中值疲劳强度σ-1约为400 MPa,优于C70S6BY钢的疲劳极限.V-N微合金钢的疲劳裂纹萌生于试样表面的铁素体-珠光体边界,并沿着铁素体-珠光体边界及珠光体内部扩展,疲劳断口呈韧窝状,属韧性断裂.C70S6BY中先共析铁素体呈薄片状断续分布在珠光体周围,疲劳裂纹在晶界铁素体处萌生及扩展,疲劳断口呈解理状,属脆性疲劳断裂.

参考文献

[1] Weber M.Cost effective finishing of power forged connecting rods with the fracture splitting method[A].,1991:1-7.
[2] Repgen B.Optimized connecting rods to enable higher engine performance and cost reduction[A].,1998:23-26.
[3] Gu Z;Yang S;Ku S et al.Fracture splitting technology of automobile engine connecting rod[J].Intermational Journal of Advanced Manufacturing Technology,2005,25:883-887.
[4] Cristinacce M;Reynolds P E;Milbourn D J.The current status of the development and use of air cooled steels for the automotive industry[A].Colorado:Colorado School of Mines,1996:1-16.
[5] Woodhead J H.Review of principles of microalloyed bar and forging steels[A].TMS,Warrendale,PA,1986:3-17.
[6] Grassl K J;Thompson S W;Krauss G.New options for steel selection for automotive applications[A].,1989:417-430.
[7] Shinsaku Fukuda;Hirohito Eto .Development of fracture splitting connecting rod[J].JSAE review,2002(1):101-104.