Nanosized amorphous TiO2 powders with a specific surface area of 501 m2.g-1 were prepared by hydrolysis. Aftercalcined at 400℃ for 2 h, the prepared amorphous TiO2 powders were fully transformed into anatase crystallitesthe samples of nanosized amorphous TiO2 mixed with microsized anatase, nanosized anatase, or nanosized α-Al2O3respectively. Effects of sample packing, anatase addition, or α-Al2O3 addition on the crystallization behavior ofnanosized amorphous TiO2 were analyzed.

参考文献

[1] B Ohtani;Y Ogawa;S.Nishimoto .[J].Journal of Physical Chemistry,1997,B101:3746.
[2] B Kraeutler;A J Bard .[J].Journal of the American Chemical Society,1978,100:5985.
[3] M V Rao;K Rajeswar;V R Pai;J Dubow .[J].Journal of Physical Chemistry,1980,84:1987.
[4] J Y Chen;L Gao;J H Huang .[J].Journal of Materials Science,1996,31:3497.
[5] D C Hague;M J Mayo .[J].Journal of the American Ceramic Society,1994,77:1957.
[6] K P Kumar;K Keizer;K Bruggraaf .[J].Nature,1992,358:48.
[7] K J D MacKenzie .[J].Transactions Journal of the British Ceramic Society,1975,74:77.
[8] S Hishita;I Muutoh;K K Koumoto;H Yanagida .[J].Ceramics International,1983,9:41.
[9] K N P Kumar;K Keizer;A J Burggraaf.[J].Journal of Materials Chemistry,1993(03):1141.
[10] HZhang;J F Banfield .[J].Journal of Materials Research,2000,15:437.
[11] Q Zhang;L Gao;d J Guo .[J].Journal of the European Ceramic Society,2000,20:2153.
[12] HZhang;J F Banfield .[J].American Mineralogist,1999,84:528.
[13] M Kumagai;G L Messing .[J].Journal of the American Ceramic Society,1985,68:500.
[14] P Nair;F Mizukami;T Okubo;J Nair and A J Burggraff .[J].Ceram Proces,1997,43:2710.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%