Mg-Ni系合金作为一种重要的Ni/MH电池负极材料, 一直受到电池工作者的广泛重视. 本文对机械合金化方法制备Mg-Ni系合金作为Ni/MH电池氢化物电极材料的研究现状进行了全面介绍, 综述了Mg-Ni系合金的电化学性能、微观结构、吸放氢机理以及合金的制备方法, 如二元合金化、多元合金化、复合合金化、表面改性等, 并就机械合金化方法制备Mg-Ni系合金作为Ni/MH电池负极材料的研究前景进行了分析和展望.

Mg-Ni based alloy has always been paid much attention as important negative electrode materials for Ni/MH battery. Recent research progress in Mg-Ni based alloy by mechanical
alloying for Ni/MH battery hydride electrode materials was reviewed with its focus on the electrochemical performance, micro-structural
characteristics, mechanism of hydriding and dehydriding and the main methods in preparation and modification of Mg-Ni based alloy electrodes such as
Mg-Ni based binary alloys, ternary alloys, composite alloying and surface modifications. Also the main direction of studies on Mg-Ni based alloy by
mechanical alloying for Ni/MH battery negative electrode materials was proposed.

参考文献

[1] Liu Weihong, Wu Haoqing, Lei Yongquan, et al. J. Alloys and Comp., 1997, 261: 289-294.
[2] Liu Weihong, Wu Haoqing, Lei Yongquan, et al. J. Alloys and Comp., 1997, 252: 234-237.
[3] Liu Weihong, Lei Yongquan, Wu Jing, et al. J. Alloys and Comp., 1996, 58: 243-247.
[4] 吴李明, 雷永泉, 吴京, 等. 稀有金属材料与工程, 1997, 26 (3): 26-29.
[5] 刘卫红, 雷永泉, 孙大林, 等. 稀有金属材料与工程, 1995, 24 (4): 33-36.
[6] Lai Y Q, Wang C S, Pan X G, et al. J. Alloys and Comp., 1995, 231: 611-615.
[7] Liu Weihong. Journal of Shanghai University(English Edition), 2002, 6 (4): 349-352.
[8] Liu Weihong, Lei Yongquan, Wu Jing, et al. Int. J. Hydrogen Energy, 1997, 22 (10/11): 999-1003.
[9] Ye H, Lei Y Q, Chen L S, et al. J. Alloys and Comp., 2000, 311: 194-199.
[10] Iwakura C, Nohara S, Zhang S G, et al. J. Alloys and Comp., 1999, 258: 246-249.
[11] Zhang S G, Hara Y, Morikawa T, et al. J. Alloys and Comp., 1999, 293-295: 552-555.
[12] 叶辉, 陈立新, 雷永泉. 稀有金属材料与工程, 2000, 29 (3): 192-196.
[13] Mu D, Hatana Y, Abe T, et al. J. Alloys and Comp., 2002, 334: 232-237.
[14] Goo Nom Hoon, Woo Jung Hoon, Lee Kyung Sub. J. Alloys and Comp., 1999, 288: 286-293.
[15] Cui N, He P, Luo J L. Electrochemical Acta., 1999, 44: 3549-3558.
[16] Woo Jung Hoon, Jung Chang Bo, et al. J. Alloys and Comp., 1999, 293-295: 556-563.
[17] 王尔德, 胡连喜. 粉末冶炼技术, 2002, 20 (3): 135-139.
[18] Tony Spassov, Uwe Koster. J. Alloys and Comp., 1998, 279: 279-286.
[19] 雷永泉. 新能源材料. 天津大学出版社, 24.
[20] 胡子龙. 贮氢材料. 化学工业出版社, 49-51.
[21] 王仲民, 曾美琴, 杨永强. 中国有色金属学报, 2001, 11 (2): 236-238.
[22] 王仲民, 彭成红, 李祖鑫. 电池, 2000, 30 (6): 266-268.
[23] 杨幼平, 张平民, 刘开宇. 金属功能材料, 2002, 9 (6): 1-4.
[24] 唐有根, 徐益军, 杨幼平. 金属功能材料(Metallic Functional Materials), 2002, 9 (3): 1-4.
[25] Liang Guoxian, Wang Erde, Fang Shoushi, et al. J. Alloys and Comp., 1995, 223: 111-114.
[26] Jung Chang Bo, Lee Kyung Sun, et al. J. Alloys and Comp, 1997, 253-254: 605-608.
[27] 郭再萍, 夏熙. 电池(Battery Bimonthly), 1998, 28 (1): 33-38. 奬re{[28] Ji S J, Sun J C, Yu Z W. International Journal of Hydrogen Energy, 1999, 24: 59-63.
[29] Liang G, Boily S, Huot J, et al. J. Alloys and Comp., 1998, 267: 302-306.
[30] 陈文革, 丁秉钧, 张晖. 中国有色金属学报, 2002, 12 (6): 1224-1228.
[31] 卢斌, 易丹青, 刘会群. 中国有色金属学报, 2002, 12 (6): 1214-1217.
[32] 马学鸣, 杨元政, 董远达. 金属学报, 1992, 28 (2): 72-74.
[33] 柴志刚, 赵敏寿. 吉林大学自然科学学报, 2000, 01: 75-76.
[34] Varin R A, Czujko T, Mizera J, et al. J. Alloys and Comp., 2003, 350: 332-339.
[35] Hong Kuochih, et al. J. Alloys and Comp, 2001, 321: 307-313.
[36] Gross Karl J, Chartouni Daniel, Leroy Eric, et al. J. Alloys and Comp., 1998, 269: 259-270.
[37] Aizawa T, Kuji T, Nakano H, et al. J. Alloys and Comp., 1999, 291: 248-253.
[38] 王尔德, 方守狮, 梁国宪. 材料科学与工艺, 1994, 2 (3): 24-27.
[39] Nohara Shinji, Fujita Naoya, Zhang Shuguo, et al. J. Alloys and Comp., 1998, 267: 76-78.
[40] Iwakura Chiaki, Ryuji Shin-ya, et al. Electrochimica Acta., 2001, 46: 2781-2786.
[41] Iwakura Chiaki, Nohara Shinji, Inoue Hiroshi. Solid State Ionics., 2002, 148: 499-502.
[42] Iwakura C, Inoue H, Nohara S, et al. J. Alloys and Comp., 2002, 330-332: 636-639.
[43] Yuan Huatang, Li Qiudi, Song Henan, et al. J. Alloys and Comp, 2003, 353: 322-326.
[44] 薛建设, 李国勋, 胡尧沁. 稀有金属, 2000, 24 (2): 124-126.
[45] Lee Hee Yong, Goo Nam Hoon, Jeong Woon Tae, et al. J. Alloys and Comp, 2000, 313: 258-262.
[46] 李金平, 王晓林, 王尔德. 兵器材料科学与工程, 1997, 20 (5): 7-11.
[47] 李金平, 王晓林, 王尔德. 材料科学与工艺, 1998, 6 (2): 69-73.
[48] Cui N, Luo J L. Electrochemical Acta., 1998, 44: 711-720.
[49] Cui N, Luan B, Zhao H J. J. Alloys and Comp., 1996, 233: 236-240.
[50] Cui N, He P, Luo J L. Acta Mater., 1999, 47 (14): 3737-3743.
[51] Cui N, Luo J L, Chuang K T. J. Alloys and Comp., 2000, 302: 218-226.
[52] Cui N, Luo J L. J. Alloys and Comp., 1998, 265: 305-310.
[53] Cui N, Luo J L. Electrochemical Acta., 2000, 45: 3973-3981.
[54] Gross Karl J, Spatz Peter, Zuttel Andreas, et al. J. Alloys and Comp., 1996, 240: 206-213.
[55] Bloch Joseph, Mintz Moshe H. J. Alloys and Comp., 1997, 253-254: 529-541.
[56] Cui N, Luo J L. International Journal of Hydrogen Energy, 1999, 24: 37-42.
[57] 王仲民, 彭成红, 欧阳柳章. 金属学报, 2002, 38 (2): 189-192.
[58] Cui N, Luan B, Liu H Ks, et al. Journal of Power Resource, 1995, 233: 263-267.
[59] Kyung Weon, Tanaka Toshiyuki, Miyauchi Rie, et al. J. Alloys and Comp., 2000, 299: 141-147.
[60] 王仲民, 朱敏, 彭成红. 中国有色金属学报, 2002, 12 (2): 300-304.
[61] Hatano Yuji, Tachikawa Tomoyuki, et al. J. Alloys and Comp., 2002, 330-332: 816-820.
[62] 闫德意, 崔涛, 程骞. 电源技术(Chinese Journal of Power Resource), 1998, 22 (5): 192-194.
[63] Chen Weixiang. Journal of power sources, 2000, 90: 201-205.
[64] Inoue Hiroshi, Hazui Shinya, et al. Electrochemical Acta., 1998, 43 (14-15): 2221-2224.
[65] Jiang Jian Jun, Gasik Michael. Journal of Power Sources, 2000, 89: 117-124.
[66] Iwakura Chiaki, Inoue Hiroshi, Zhang Shu G, et al. J. Alloys and Comp., 1999, 293-295: 653-657.
[67] Funaki Keiji, Orimo Shin-ichi, Fujii Hironobu, et al. J. Alloys and Comp., 1998, 270: 160-163.
[68] Stephane Ruggeri, Lionel R, Jacques Huot, et al. J. Alloys and Comp., 2002, 313: 170-178.
[69] Abe Takayuki, Inoue Sachio, Mu Daobin, et al. J. Alloys and Comp., 2003, 349: 279-283.
[70] Luo J L, Cui N. J. Alloys and Comp., 1998, 264: 299-305.
[71] Zhang Shuguo, Yorimitsu Kenshi, Nohara Shinji, et al. J. Alloys and Comp., 1998, 270: 123-126.
[72] Nohara Shinji, Inoue Hiroshi, Fukumoto Yukio, et al. J. Alloys and Comp., 1997, 259: 183-185.
[73] Hayashi Shigenobu, Nowak Bogdan, et al. J. Alloys and Comp., 1997, 256: 159-165.
[74] Wang C S, Wang X H, Lei Y Q, et al. Int. J. Hydrogen Energy., 1997, 22 (12): 1117-1124.
[75] Liu Weihong, Wu Haoqing, Lei Yongquan, et al. J. Alloys and Comp., 2002, 346: 244-249.
[76] Cui N, Luo J L, Chuang K T, et al. J. Alloys and Comp., 2001, 503: 92-98.
[77] 张耀, 孙俊才, 季世军. 中国有色金属学报, 2000, 10 (6): 882-886.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%