欢迎登录材料期刊网

材料期刊网

高级检索

以分析纯Na_2CO_3,K_2CO_3和Nb_2O_5为原料,以Na_2CO_3-K_2CO_3(摩尔比1: 1)为熔盐,采用熔盐法在700~850 ℃保温4 h合成了Na_(0.5)K_(0.5)NbO_3粉体.研究了合成温度、熔盐含量对粉体形貌的影响.XRD分析结果表明:通过熔盐法可以在700 ℃下合成纯钙钛矿结构的Na_(0.5)K_(0.5)NbO_3粉体;SEM分析显示:随着合成温度的升高,粉体形貌从圆球状转变为立方状,进一步提高合成温度,粉体形貌开始变得不规则;此外,合成粉体的尺寸随着熔盐含量的增加而增大,且粉体团聚现象明显减弱.以熔盐法合成的Na_(0.5)K_(0.5)NbO_3粉体为原料,采用传统固相烧结法制备Na_(0.5)K_(0.5)NbO_3陶瓷,经1060 ℃烧结后,Na_(0.5)K_(0.5)NbO_3陶瓷具有优异的压电性能和介电性能,其中压电常数d_(33) =124 pC/N,介电常数ε_(33)~T/ε_0 = 345,居里温度T_c 达 402 ℃.

参考文献

[1] 贺连星,李毅,李广成,李承恩.无铅压电陶瓷材料研究进展[J].电子元件与材料,2004(11):52-55.
[2] Takenaka T;Huzumi A;Hata T et al.Mechanical Properties of (BiNa)_(1/2)TiO_3-based Piezoelectric Ceramics[J].Silicates Industries,1993,7(08):136-142.
[3] Takenaka T;Sakata K;Toda K .Piezoelectric Properties of (BiNa)_(1/2)TiO_3-based Piezoelectric Ceramics[J].Ferroelectrics,1990,106:375-380.
[4] 赁敦敏,肖定全,朱建国,余萍,鄢洪建.无铅压电陶瓷研究开发进展[J].压电与声光,2003(02):127-132.
[5] 廖润华,李月明,江向平,王竹梅,张玉平.溶胶-凝胶法制备Na0.5Bi0.5TiO3-K0.5Bi0.5TiO3体系无铅压电陶瓷的研究[J].人工晶体学报,2008(03):652-656.
[6] 陈燕,江向平,涂娜,冯子义,陈超,李月明.K_4CuNb_8O_(23)掺杂对K_(0.44)Na_(0.52)Li_(0.04)Nb_(0.86)Ta_(0.10)Sb_(0.04)O_3压电陶瓷性能的影响[J].人工晶体学报,2009(05):1098-1102.
[7] Saito Y;Takaol H;Tani T et al.Lead-free Piezoceramics[J].NATURE,2004,432(04):84-87.
[8] Yiping Guo;Ken-ichi Kakimoto;Hitoshi Ohsato .Dielectric and piezoelectric properties of lead-free (Na_(0.5)K_(0.5))NbO_3-SrTiO_3 ceramics[J].Solid State Communications,2004(5):279-284.
[9] 杜红亮,李智敏,周万城,屈绍波,裴志斌.(Na0.5K0.5)NbO3基无铅压电陶瓷的研究进展[J].无机材料学报,2006(06):1281-1291.
[10] Yoon KH.;Kang DH.;Cho YS. .Molten salt synthesis of lead-based relaxors [Review][J].Journal of Materials Science,1998(12):2977-2984.
[11] Yanmei K;Jin X H;Wang P L et al.Anisotropic Gain Growth of Bi_4Ti_3O_(12) in Molten Salt Fluxes[J].Materials Research Bulletin,2003,38:567-576.
[12] 蔡宗英,邢献然,邓金侠,于然波,刘桂荣.熔盐快速合成Pb1-xLaxTiO3粉体[J].无机化学学报,2006(08):1421-1425.
[13] Cahn J W.On the Morphology Stability of Growth Crystals in Crystal Growth[M].UK:Pergamon,Oxford,1967:88-95.
[14] Duran C.;McKinstry S.T. .Fabrication and Electrical Properties of Textured Sr_(0.53)Ba_(0.47)Nb_2O_6 Ceramics by Template Grain Growth[J].Journal of the American Ceramic Society,2000(9):2203-2213.
[15] Maeder M D;Damjanovic D;Setter N .Lead-free Piezoelectric Materials[J].Journal of Electroceramics,2004,13:385-387.
[16] Guo Y;Kakimoto K;Ohsato H .Structure and Electrical Properties of Lead-free (K_(0.5)Na_(0.5))NbO_3-BaTiO_3 Ceramics[J].Japanese Journal of Applied Physics,2004,43:6662-6666.
[17] Fan Y H;Sun Q C;Wang Y B et al.The Preparation of (K_(0.5)Na_(0.5))NbO_3 Powder by Molten Salt Synthesis[J].Functional Materials,2005,12(36):1974-1976.