Fe-6.5wt%Si composite compact was fabricated by spark plasma sintering(SPS).Mechanical alloying(MA)was used to prepare Fe-Si composite powders.The composite powders were sintered by SPS at elevsated temperature from 500℃ to 700℃.The experimental results indicate that the non-equilibrium state of composite Fe-Si is preserved in the compact.The density of the bulk rises with the increasing temperature and there is no diffusion of silicon and iron in the interface.

参考文献

[1] G E Fish;C F Chang;R Bye .Frequency Dependence of Core Loss in Rapidly Quenched Fe-65wt%Si[J].Journal of Applied Physics,1988,64(10):5370-5372.
[2] Y Tanaka;Y Takada;M Abe;S Masuda .Magnetic Properties of 65%Si-Fe Sheet and Its Applications[J].Journal of Magnetism and Magnetic Materials,1990,83:375-376.
[3] Kenji Narita;Masato Enokizono .Effect of Nickel and Manganese Addition on Ductility and Magnetic Properties of 65% Silicon-Iron Alloy[J].IEEE Transactions on Magnetics,1978,14(04):258-262.
[4] N. Stevulova;A. Buchal .Structural investigation of the high-energy milled Fe-Si system[J].Journal of Magnetism and Magnetic Materials,1999(0):190-192.
[5] Roberto Martinez Sanchez;Francisco Espinosa Magana;Alberto Duarte Moller;Jose Gerardo Cabanas Moreno;David Rios Jara;Yoshito Nishikawa;Sebastian Diaz De La Torre .Metastability of mechanically alloyed and spark plasma sintered Co{sub}50Ti{sub}50 powder[J].粉体および粉末冶金,2000(5):480-483.
[6] 张东明,傅正义.放电等离子加压烧结(SPS)技术特点及应用[J].武汉工业大学学报,1999(06):15-17.