欢迎登录材料期刊网

材料期刊网

高级检索

The Nd2Fe14B grain growth kinetics in sintered NdFeB magnets with nominal compositions of Nd30+xDy1.5Fe67.08-xAl0.4B1.02 (%, x=0, 3) was studied. The grain size parameters were determined by means of the linear intercept method on SEM secondary electron images. It is observed that the grain growth process is more sensitive to sintering temperature than to sintering time although the grain size rises with both sintering temperature and time. It is also found that magnets prepared from the pre-alloy powder with a higher oxygen content exhibit a lower grain growth rate and magnets made from the pre-alloy powder with a broader particle size distribution demonstrate a higher grain growth rate. It is believed that the presence of appropriate amounts of Nd oxides effectively impedes the grain growth process and a larger difference in sizes between pre-alloy powder particles significantly accelerates the grain growth process. On the basis of experimental results, the grain growth exponent and the corresponding activation energy were obtained. A possible grain growth mechanism in NdFeB magnets during sintering was briefly discussed.

参考文献

[1] Sagawa M;HIROSAWA S;YAMAMOTO H et al.Nd-Fe-B permanent magnet materials[J].Japanese Journal of Applied Physics,1987,26:785-800.
[2] Wecker J;CERVA H;KUHRT C et al.Microstructure and magnetic properties of mechanically alloyed anisotropic Nd-Fe-B[J].Journal of Applied Physics,1994,76(10):6238-6240.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%