以Ca(NO3)2·4H2O、P2O5和Zn(N03)2·6H2O的乙醇溶液为原料,用溶胶凝胶法合成含锌羟基磷灰石(Zn-HA)粉体.采用X-射线衍射(XRD)、透射电镜(TEM)、红外光谱(FTIR)、热重差热(TG-DTA)对Zn-HA的晶相、形貌、化学组成和热稳定性进行了分析.结果表明:锌取代部分钙进入HA的晶格中降低了磷灰石的颗粒尺寸;当锌含量低于40%时,不会改变HA的晶体结构,但因锌离子半径小于钙离子半径,导致HA的结晶度降低,微晶尺寸减小.TG-DTA分析表明,锌掺入降低姒的热稳定性.

参考文献

[1] Mayer I;Featherstone J D B .[J].Journal of Crystal Growth,2000,219:98.
[2] Okazaki M. .CRYSTALLOGRAPHIC PROPERTIES OF HETEROGENEOUS MG-CONTAINING FLUORIDATED APATITES SYNTHESIZED WITH A TWO-STEP SUPPLY SYSTEM[J].Biomaterials,1995(9):703-707.
[3] Gibson I R;Bonfield W .[J].Journal of Materials Research,2002,59(04):697.
[4] Bertoni E.;Bigi A.;Cojazzi G.;Gandolfi M.;Panzavolta S.;Roveri N. .Nanocrystals of magnesium and fluoride substituted hydroxyapatite[J].Journal of Inorganic Biochemistry: An Interdisciplinary Journal,1998(1/2):29-35.
[5] Beattie J H;Alison A .[J].Nutrition Research Reviews,1992,5:167.
[6] Yamaguchi M;Oishi H;Suketa Y .[J].Biochemical Pharmacology,1987,36(22):4007.
[7] Moonga B S;Dempster Q W .[J].J Bone Miner Tes,1995,10(03):453.
[8] Grandjean-Laquerrierea A;Laquerriere P;Jallot E et al.[J].Biomaterials,2006,27:3195.
[9] Jallot E;Nedelec J M;Grimault A S et al.[J].Colloids and Surfaces B:Biointerfaces,2005,42:205.
[10] Miao SD;Weng WJ;Cheng K;Du PY;Shen G;Han GR;Zhang S .Sol-gel preparation of Zn-doped fluoridated hydroxyapatite films[J].Surface & Coatings Technology,2005(1/3):223-226.
[11] Miyaji F;Kono Y;Suyama Y .[J].Materials Research Bulletin,2005,40(02):209.
[12] Fujii E;Ohkubo M;Tsuru K et al.[J].Acta Biomaterialia,2006,2:69.
[13] LeGeros R Z;Bleiwas C B;Retino M et al.[J].American Journal of Dentistry,1999,12:65.
[14] Bouyer E;Gitzhofer F;Boulos I .[J].Journal of Materials Science:Materials in Medicine,2000,11:523.
[15] Baddielang C B;Berry E E .[J].J Spectro Chim Acta,1996,22:1407.
[16] Gonzalez-diaz P F;Sandtos M .[J].Journal of Solid State Chemistry,1997,22:193.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%