In the present work investigations have been made to see the role of metal oxides on the performance of the silver metal oxides electrical contact materials. Silver metal oxide materials of three different compositions Ag-10CdO, Ag7.6SnO2-2.3In2O3 and Ag-10ZnO were prepared by internal oxidation process under identical processing conditions.These materials were tested for electrical conductivity, hardness, and erosion loss. Performing an accelerated test on the actual contactor assessed the electrical performance, involving erosion loss and temperature rise of the processed materials. The arc-eroded surface was characterized under scanning electron microscope. The study of the eroded surfaces of contacts indicates that the thermal stability of metal oxides depends on nature of silver-metal oxide interface and their mode of erosion. An attempt is made to correlate the surface features of the eroded contacts with the thermal stability of metal oxides.

参考文献

[1] E Vinaricky;U Harmsen .[J].Metall,1971,25:749.
[2] W Kunert;G HauBler;H Scheibe.[A].on Electrical Contact Phenomena Tokyo,1976:143.
[3] M.Iida .[Q].
[4] M Sato;M Hijikata;I Morimoto .[Q].Ibid
[5] F R Hensel .[P].US No 2145690,1939.
[6] C D DesForges .[J].Powder Metallurgy,1979,3:138.
[7] M Sato;M Hijikata .[J].Materials Transactions,1982,23(05):267.
[8] P C Wingert;C H Leung .[J].IEEE Transactions on Components Hybrids and Manufacturing Technology,1989,12(01):16.
[9] A Verma;A Roy;T R Anantharaman .[J].International Journal of Powder Metallurgy,1991,27:51.
[10] A Verma .[J].Journal of Powder Metallurgy and Powder Technology,1993,5:16.
[11] C.J.Gao.[A].北京,1989:193.
[12] G Jiacong.[J].Ibid:215.
[13] D.Brenner;M.Huck;R.Michal;K.E.Saeger .[Q].
[14] Y.S.Shen;L.Gould.[A].,1987:157.
[15] P C Wingert;C H Leung.[J].IEEE Transactions on Components Hybrids and Manufacturing Technology,1987(10):63.
[16] J Amier;M J Frabcukkib;D Jeannot;P Ramoni and J C Ramseyer.[A].on Electric Contacts Switzerland,1986:206.
[17] P C Wingert;C H Leung.[A].on Electrical Contacts,1986:63.
[18] Y S Shen;L Gould.[A].on Electrical Contacts,1984:193.
[19] G Petzow;G.Effenberg .in Ternary Alloys A Com Prehensive Compendium of Evaluated Constitutional Data and Phase Diagrams[M].VCH Publishers,1988,2:314.
[20] E.A.Brandes.Smithells Metals Reference Book[M].Butter-worths:198311-26.
[21] A Verma;T R Anantharaman .[J].Bulletin of Marine Science,1991,14(01):1.
[22] T Igarashi;Y J Kodama .[J].Journal of the Materials Science Society of Japan,1979,16:212.
[23] T Tigarashi;M Shibata;Y Kodama .[J].Journal of the Japan Institute of Metals,1980,44:378.
[24] W.Bohn;M.Lindmayer;M.Classing.[A].,1980:51.
[25] K.Sakairi;H.Tsuji;K.Tsuchiya.[A].,1982:77.
[26] K H Schroder .[J].IEEE Transactions on Components Hybrids and Manufacturing Technology,1987,10:127.
[27] H.Yamasaki;S.Oda;K.Miyakawa.[A].,1980:799.
[28] N.Behrens;W.Bohm;P. Braumann;G.Klepp.[A].,1984:185.
[29] U.Mayer;R.Michal;E.K.Saeger .[Q].Ibid
[30] N.Behrens;W.Bohm.[A].,1982:203.
[31] R M K Young;T W Clyne .[J].Acta Materialia,1989,37:663.
[32] F S rugner.[J].Proc of Holm Seminar on Electrical Contacts,1977:77.
[33] D.J.Pedder;F.S.Brugner.[C].Proc of Holm Seminar on Electrical Contacts,1975:47.
[34] Y K Lee;Thomas J O Keefe .[J].OM,2002,54(04):12.
[35] P.Ramachandrarao;S.N.Ojha;O.P.Pandey .[J].Philosophical Magazine Letters,1992,66:33.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%