制备了双组份水性聚氨酯木器涂料,探讨了羟基组分聚丙烯酸酯(PA)含量和固化剂用量对涂膜强度以及耐溶剂性、硬度和抗冲击性能等影响,并根据粒径分析和透射电子显微镜(TEM)等测试方法研究了羟基聚氨酯-丙烯酸酯复合乳液(PUA)和固化剂的反应情况及树脂结构。结果表明,PA含量为15%,固化剂加入量为5%时得到稳定性、涂膜硬度、韧性、耐溶剂性较优的水性聚氨酯木器涂料。

In this paper,two component waterborne polyurethane wood coating were obtained by hydroxyl polyurethane-acrylate(PUA) composite dispersion with synthesized curing agent.The influences of acrylate(PA) content and curing agent on the paint film properties were investigated by particle size analysis and transmission electron microscopy(TEM),respectively.It was found that when the content of PA is 15% and the curing agent is 5%,the waterborne polyurethane wood coating obtained better emulsion stability,hardness,toughness,impact resistance and more excellent solvent resistance.

参考文献

[1] 伍忠岳,叶荣森,刘志刚.双组分水性木器涂料发展现状及存在问题[J].中国涂料,2008(01):9-11.
[2] 伍忠岳,叶荣森,刘志刚.含-NCO双组分水性木器漆的应用研究[J].现代涂料与涂装,2008(02):24-26.
[3] 邓朝霞,叶代勇,黄洪,陈焕钦.环氧树脂改性水性聚氨酯的合成研究[J].功能材料,2007(07):1132-1135.
[4] 刘瑞源,瞿金清,谢扬,陈焕钦.水性木器涂料的新进展[J].化学工业与工程,2003(02):89-94.
[5] 王小荣,沈一丁,赖小娟.γ-(甲基丙烯酰氧基)丙基三甲氧基硅烷改性聚氨酯的研究[J].功能材料,2011(10):1814-1816,1820.
[6] 杜茂平;毛君绒;曾睿 .[J].涂料涂装与电镀,2006,4(05):11-13.
[7] Werner J B;Jtramontano V .[J].Progress in Organic Coatings,1996,27(1-4):1-15.
[8] Sukop S .[J].Leather Science and Engineering,2006,16(02):3-7.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%