合成了HA/PU复合膜在体外进行了试验评估,用IR、XRD、SEM和ICP等手段对材料组成,降解性和表面形貌进行了分析以及对吸水率和失重率的测定,结果表明,HA/PU膜在浸泡过程中,在去离子水中不但发生了水解,在SBF溶液中还发生了Ca,P的沉积,使得复合膜不但具有一定的降解性,还表现出一定的生物活性,表面出现的多孔,为细胞的培养奠定了基础,在骨修复或替代材料中具有一定的价值.

参考文献

[1] Bernacca GM.;Wilkinson R.;Wheatley DJ.;Mackay TG. .CALCIFICATION AND FATIGUE FAILURE IN A POLYURETHANE HEART VALVE[J].Biomaterials,1995(4):279-285.
[2] Mackay TG.;Bernacca GM.;Fisher AC.;Hindle CS.;Wheatley DJ. .NEW POLYURETHANE HEART VALVE PROSTHESIS - DESIGN, MANUFACTURE AND EVALUATION[J].Biomaterials,1996(19):1857-1863.
[3] Szycher M;Poirier V;Dempsey D.Applied Mechanics Division[M].Boston:American Society of Mechanical Engineers,1979:743-747.
[4] Blamey J;Rajan S;Unsworth A et al.[J].Annals of Biomedical Engineering,1991,13(03):180-184.
[5] Kaibara M.;Yanagida S.;Kawakami S.;Kawamoto Y. .IN VITRO EVALUATION OF ANTITHROMBOGENICITY OF HYBRID-TYPE VASCULAR VESSEL MODELS BASED ON ANALYSIS OF THE MECHANISM OF BLOOD COAGULATION[J].Biomaterials,1995(16):1229-1234.
[6] Gorna K;Gogolewski S .Biodegradable porous polyurethane scaffolds for tissue repair and regeneration.[J].Journal of biomedical materials research, Part A,2006(1):128-138.
[7] Desai S D;Emanuel A L et al.[J].Journal of Polymer Research,2003,10:275-281.
[8] Dahiyat B I;Posadas E M;Hirosue S et al.[J].Reactive Polymers,1995,25:101-109.
[9] Ozgurengin N;Cuneyttas A .[J].The European Ceramics Society,1999,19:2569-2572.
[10] Hollinger J O;Battistone G C .[J].Clinical Orthopaedics & Related Research,1986,207:290-305.
[11] Hammerle C H;Olah A J;Schmid J et al.[J].Clinical Oral Implants Research,1997,8:198-207.
[12] Yuan Huipin;Kurashina K;de Bruijn J D et al.[J].Biomaterials,1999,20:1799-1806.
[13] Wei Jie;Li Yubao .[J].European Polymer Journal,2004,40:509-515.
[14] Kokubo T;Kushitani H;Sakka S et al.[J].Journal of Biomedical Materials Research,1990,24(06):721-734.
[15] 美国材料协会;奚廷斐;赵黎力.ASTM标准年监(医用装置标准13.01卷)[M].成都:成都科学技术大学出版社,1990:70.
[16] LeGeros R Z;Daculsi.Monographs in Oral Science[M].Biphasic:Reed Health Care Communication Press,1992:201.
[17] 刘凉冰 .[J].弹性体,1995,5(03):39.
[18] 李仙会,庞坤玮,韩雷岗.聚氨酯弹性体的降解及其稳定剂[J].聚氨酯工业,2000(02):1-4.
[19] Spaans CJ.;Rienstra O.;de Groot JH.;Veth RPH.;Pennings AJ.;Belgraver VW. .Solvent-free fabrication of micro-porous polyurethane amide and polyurethane-urea scaffolds for repair and replacement of the knee-joint meniscus[J].Biomaterials,2000(23 Special Issue SI):2453-2460.
[20] Zhang S W;He Renyang;Wang Deguo.[J].Journal of Materials Science,2001(36):5037-5043.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%