欢迎登录材料期刊网

材料期刊网

高级检索

通过对16Cr14Co12Mo5轴承钢经冷处理后的组织和性能进行研究,发现与淬火态相比,试验钢经两次冷处理和高温回火后,表面硬度达到50.7HRC,抗拉强度Rm达到1 820MPa,屈服强度Rp0.2达到1 410MPa,冲击功为75.0J,试验钢的强度和硬度得到了显著提高。经XRD检测,经过两次冷处理后残余奥氏体体积分数由26.0%下降到3.1%。研究表明,经过2次冷处理并配合高温回火后,钢中残余奥氏体88.1%转变为马氏体,残余奥氏体含量明显降低,组织变得稳定,并且在回火过程中伴随有一定量微细第二相的析出。

The microstructure and mechanical properties of cold treatment 16Cr14Co12Mo5 bearing steel was investigated.Compared to the quenching state,experimental steel through two cold treatment and high tempering,the surface hardness reached 50.7HRC,the tensile strength Rm reached 1 800 MPa and yield strength Rp0.2 reached 1 400 MPa,the values of ballistic work was 75.0 J,the strength and hardness of experimental steel had been significantly enhanced.By XRD detection,after twice cold treatment austenite content dropped from 26.0% to 3.1%.This results show that after cold treatment and the high tempering,in steel 80% of austenite transformed into martensite,austenite content is significantly reduced,organization becomes more stable,and a certain amount of fine second phases can be separated out in the process of tempering.

参考文献

[1] Crawfird W M;Contractor G P .The Effects of Strengthening Be and Ti in Maraging Stainless Steel[J].JIPI,1969,207(12):1642.
[2] 王康,杨卯生,樊刚,俞峰,鲍俭,闫文凯.16Cr14Co12Mo5耐热耐蚀轴承钢强韧化机制的研究[J].钢铁,2011(10):75-79.
[3] 陈鼎,刘芳,滕杰,杨芳,陈振华.深冷处理对低碳钢组织与性能的影响[J].金属热处理,2008(09):66-69.
[4] 刘耀中,左传付.轴承钢零件淬回火后的残余奥氏体[J].轴承,2008(06):48-51.
[5] 翟应田;彭匡鼎;姚裕昌 等.深冷处理中钢铁机制强化的物理机理[J].云南大学学报(自然科学版),1996,18(03):226.
[6] 姜明,黄敏纯,黄蔚平,章嘉琼.超低温温度场中轴承钢显微组织转变对机械性能的影响[J].江南大学学报(自然科学版),2008(02):203-206.
[7] 钱士强,童建华,马宁,陆蓉.原位观察深冷处理板条马氏体[J].热加工工艺,2008(08):12-14.
[8] 段春争,王敏杰,李士燕.深冷处理工艺对W6Mo5Cr4V2钢力学性能和微观组织的影响[J].材料工程,2008(06):40-43.
[9] 鲍俭,杨卯生,王华昆.热处理工艺对20Cr14Co12Mo5轴承钢力学性能的影响[J].钢铁,2010(01):91-95.
上一张 下一张