通过波动拉伸载荷试验(F-SSRT),研究了不同应变速率对X70管线钢在阴极电位下近中性介质应力腐蚀开裂(SCC)行为的影响.结果表明:X70管线钢在特定的近中性介质中,在波动拉伸载荷和阴极电位(-850 mVscE)条件下,存在SCC敏感性.在波动拉伸载荷试验条件下,SCC裂纹的扩展机理与匀速慢拉伸试验时不同,SCC裂纹可以从材料表面产生的微孔处萌生并沿主应力面扩展,当应变速率在一定范围时,SCC裂纹转变为沿45°最大剪应力面扩展.还分析了波动拉伸载荷试验中氢在X70管线钢SCC发展过程中的作用和机理.

参考文献

[1] Delanty B;O'Brien J .Major Field Study Compares Pipeline Stress Corrosion Cracking With Coatings[J].Oil & Gas Journal,1992,90(24):39.
[2] Parkins R N;Alexandridou A;Majumdar P .Stress Corrosior Cracking of C-Mn Steels in Environments Coating Carbon Dioxide[J].Materials Performance,1986,25(10):10.
[3] Nishimura R;Kudo K .Stress Corrosion Cracking of AISI 304 and AISI 316 Austenitic Stainless Steels in HCI and H2SO4 So lutions-Prediction of Time-to-Failure and Criterion for Assessment of SCC Susceptibility[J].CORROSION,1989,45(04):308.
[4] Wilmott M J;Surtherby R L.The Role of Pressure and Pressure Fluctuations in the Growth of Stress Corrosion Cracks in Line Pipe Steels[A].USA:ASME,1998:409.
[5] 赵明纯,单以银,李玉海,杨柯.显微组织对管线钢硫化物应力腐蚀开裂的影响[J].金属学报,2001(10):1087-1092.