薄壁纯锆U形管在弯制过程中容易产生椭圆度、回弹、划伤以及弯管内弧褶皱等现象,为了实现小弯曲半径薄壁锆管的弯制成形,根据U形管的弯制特点,并结合实际弯制经验,设计并制作了U形管的弯制模具。该弯制模具主要采用绕管方式进行弯制,U形管一端固定,另一端进行弯制。弯制试验结果表明,该弯制模具能够制作弯曲半径为50 mm和105 mm的φ25.4 mm ×1.24 mm薄壁锆U形管,弯制后的U形管成形状态良好,检测结果均能满足GB 151—1999标准及设备生产工艺的要求,并能有效地保证弯管质量。

It is easy to ellipse , rebound, scratch and internal fold during the bending process of thin walled pure zirconium U shape tube .In order to bend of thin-walled pure zirconium tube with small bending radius , the bending die of U shape pipe is designed according to the characteristics and experience of U shape tube bending .The bending die was functioned in the way of winding , the end of the U shape tube was fixed and the other end was used to bend . The results of bending test show that the die can bend φ25.4 mm ×1.24 mm thin walled pure zirconium U shape tubes with bending radius of 50 mm and 105 mm.The U shape tubes have good forming condition , and test results can meet the requirements of GB 151—1999 standard and production process of equipment , and also can ensure the quality of tube effectively .

参考文献

[1] 王中武.U形管式换热器换热管的弯制工艺[J].化工机械,2000(04):230.
[2] NB/T 47014-2010.锆制压力容器[S].北京:中国标准出版社,2010.
[3] 孟静,赵新爱,吴胜敏,杨博.U型换热管的弯制工艺研究[J].化工装备技术,2010(02):37-39.
[4] 张方正.小弯曲半径U形管弯制工艺及质量控制[J].安庆石化,1993(1):36-37.
[5] GB 151-1999.管壳式换热器[S].北京:中国标准出版社,1999.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%