本文建立了基于磁性微球表面氨基的荧光胺定量检测方法,通过研究荧光胺与磁性微球表面氨基反应的光学性质,优化了影响检测反应的条件。碱性条件下微球表面改性氨基硅烷在反应60h后基本可从微球表面完全解离下来,荧光胺分子与解离后的游离氨基反应20min即可得到稳定的荧光信号。我们发现缓冲溶液的pH值在8.0时所得到的荧光测试信号较稳定。所建立的方法操作简便快捷,结果的准确性较高。

Fluorescamine quantitative detection method for detecting the density of surface amino groups of magnetic microspheres was established and the reaction conditions were optimized via the investigation of the optical reaction properties between fluorescamine and amino groups.It is found that the modified aminosilane carrying amino groups will be completely dissociated from the surfaces of microspheres after 60h under alkaline conditions,which renders a stable fluorescent signal after a further reaction of 20min with fluorescamine.It is shown that the fluorescent signal is most stable with pH of 8.0 in the reaction system.The detection method of the density of amino groups on magnetic microspheres based on fluorescamine is simple and fast with a high accuracy.

参考文献

[1] Pedro T et al.The preparation of magnetic nanoparticles for applications in biomedicine[J].Journal of Physics D: Applied Physics,2003,36:182-197.
[2] Yoza B;Arakaki A;Matsunaga T .DNA extraction using bacterial magnetic particles modified with hyperbranched polyamidoamine dendrimer[J].Journal of Biotechnology,2003(3):219-228.
[3] Wenru Zhao;Jinlou Gu;Lingxia Zhang;Hangrong Chen;Jianlin Shi .Fabrication of Uniform Magnetic Nanocomposite Spheres with a Magnetic Core/Mesoporous Silica Shell Structure[J].Journal of the American Chemical Society,2005(25):8916-8917.
[4] Xu, QF;Xu, H;Gu, HC;Li, JB;Wang, YY;Wei, M .Development of lateral flow immunoassay system based on superparamagnetic nanobeads as labels for rapid quantitative detection of cardiac troponin I[J].Materials science & engineering, C. Biomimetic and supramolecular systems,2009(3):702-707.
[5] Zhang, GX;Liu, YB;Zhang, CF;Hu, WQ;Xu, WB;Li, Z;Liang, S;Cao, JQ;Wang, YX .Aqueous immune magnetite nanoparticles for immunoassay[J].Journal of nanoparticle research: An interdisciplinary forum for nanoscale science and technology,2009(2):441-448.
[6] TAKESHI YAMAUCHI;AKIRA YUUKI;GANGWEI;KUMI SHIRAI;KAZUHIRO FUJIKI;NORIO TSUBOKAWA .Immobilization of Flame Retardant onto SilicaNanoparticle Surface and Properties of Epoxy Resin Filledwith the Flame Retardant-Immobilized Silica[J].Journal of Polymer Science, Part A. Polymer Chemistry,2009(22):6145-6152.
[7] Shengxiang Ji;Thomas R. Hoye;Christopher W .Macosko Primary Amine ( NH2 ) Quantification in Polymers Functionality by 19F NMR Spectroscopy[J].Macromolecules,2005,38(11)
[8] Maus, L;Spatz, JP;Fiammengo, R .Quantification and Reactivity of Functional Groups in the Ligand Shell of PEGylated Gold Nanoparticles via a Fluorescence-Based Assay[J].Langmuir: The ACS Journal of Surfaces and Colloids,2009(14):7910-7917.
[9] d'Orlye F;Varenne A;Georgelin T;Siaugue JM;Teste B;Descroix S;Gareil P .Charge-based characterization of nanometric cationic bifunctional maghemite/silica core/shell particles by capillary zone electrophoresis.[J].Electrophoresis,2009(14):2572-2582.
[10] M. Weigele;S.L. DeBernardo;J.P. Tengi;W.Leimgruber .Novel reagent for the fluorometric assay of primary amines[J].Journal of the American Chemical Society,1972,94:5927.
[11] Mahsa Ghasemi;Michel Minier;Michael Tatoulian .Determination of Amine and Aldehyde Surface Densities: Application to the Study of Aged Plasma Treated Polyethylene Films[J].Langmuir: The ACS Journal of Surfaces and Colloids,2007(23):11554-11561.
[12] Hanna Ritter;Minna Nieminen;Maarit Karppinen .A comparative study of the functionalization of mesoporous silica MCM-41 by deposition of 3-aminopropyltrimethoxysilane from toluene and from the vapor phase[J].Microporous and Mesoporous Materials,2009(1/3):79-83.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%