以低分子量聚丙烯酸钠(PAAS)为基础,将聚丙烯酸钠、钼酸钠、D-葡萄糖酸钠、苯并三氮唑、六次甲基四胺等物质按一定比例复配成无磷缓蚀阻垢剂配方,采用碳酸钙沉积法评价其阻垢性能,用旋转挂片法和电化学法评价其缓蚀性能。优选出的最佳缓蚀剂配方为:聚丙烯酸钠15mg/L、D-葡萄糖酸钠14mg/L、苯并三氮唑13mg/L、钼酸钠18mg/L、六次甲基四胺14mg/L,其阻垢率为92.63%,缓蚀率为92.78%。该配方具有无磷、无毒、高效、环保等特点,具有重要的经济和利用价值。
Based on the low molecular weight sodium polyacrylate(PAAS),the corrosion and scale inhibitor with non-phosphorus formula was prepareded by PAAS,sodium molybdate,D-glucose acid sodium,1,2,3-benzotriazole and hexamethylenetetramine in definite proportion.Its anti-scaling performance was evaluated by calcium carbonate deposition method,its corrosion inhibition was evaluated by rotation specimen method and electro chemical method.The best formula is sodium polyacrylate 15 mg/L,D-glucose acid sodium 14 mg/L,1,2,3-benzotriazole 13 mg/L,sodium molybdate 18 mg/L,hexamethylenetetramine 14 mg/L.The scale inhibition efficiency and corrosion inhibition efficiency of the inhibitor were 92.63% and 92.78% respectively.This formula ethibits the characteristics of no phosphorus,non-toxicity,high efficiency and being environmental friendly.There are important economic and use values.
参考文献
[1] | 沈翔,曾德芳,张伟.一种循环冷却水无磷缓蚀阻垢剂的研制及其性能研究[J].清洗世界,2011(09):14-19. |
[2] | Choi DJ.;You SJ.;Kim JG. .Development of an environmentally safe corrosion, scale, and microorganism inhibitor for open recirculating cooling systems[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2002(1/2):228-235. |
[3] | 胡晓静,刘振法,武秀丽,高玉华.环境友好型缓蚀阻垢剂的研制及性能研究[J].水处理技术,2010(03):38-41. |
[4] | 闫美芳,刘振法,董倩倩,张利辉,郝青.多功能环保型缓蚀阻垢剂的研制及性能研究[J].工业水处理,2011(07):64-66,70. |
[5] | 刘国华,奚旦立,李燕,陆柱.环保型无磷复合水处理剂的研制[J].腐蚀与防护,2003(11):480-482. |