高级检索

从分析凝胶注模成型陶瓷悬浮体的固化机制入手总结了陶瓷坯体内应力产生的根源,并从缺陷控制角度指出,内应力在陶瓷坯体中的遗传和发展容易导致宏观裂纹的产生.通过改善凝胶体系来调控高分子网络,如利用丙烯酸羟乙酯与丙烯酰胺的共聚,或者在陶瓷浓悬浮体中添加适量聚乙二醇增塑陶瓷坯体可有效控制和消除陶瓷坯体中的内应力.

In this article,the origin of the internal stress in the ceramic green bodies is concluded by analyzing the solidification of concentrated ceramic suspension during the gelcasting. Furthermore,from the point of view of the defect's controlling,it's indicated that the inheriting and varying of the internal stress during the ceramic green body can result in the macro crack easily. Adjusting polymer network structure by designing new gel-system is a valid method of removing the internal stress. Copolymerization between hydroxyl-ethyl-acrylate and acrylamide,or adding proper polyethylene glycol into the concentrated ceramic suspension,both can reduce or avoid internal stress in the green body effectively.

参考文献

[1] Huang Y et al.A new approach to prepare high-performance ceramic parts with complex shapes:Aqueous injection molding[J].Key Engineering Materials,2003,247:39.
[2] Lange F F .Powder processing science and technology for increased reliability[J].Journal of the American Ceramic Society,1989,72(01):3.
[3] Young A C;Omatete O O;Janney M A et al.Gelcasting of alumina[J].Journal of the American Ceramic Society,1991,74(03):612.
[4] 马利国,杨金龙,张立明,黄勇.煅烧预处理改善氮化硅的凝胶注模成型工艺[J].硅酸盐通报,2004(01):13-16.
[5] 马天,孙艳荣,赵雷,杨金龙,黄勇.臭氧发生器用金红石陶瓷薄壁管的研制[J].硅酸盐通报,2008(01):46-49,54.
[6] Gilissen R;Erauw J P;Smolders A et al.Gelcasting,a near net shape technique[J].Materials & Design,2000,21(04):251.
[7] Yang J et al.Direct coagulation casting via increasing ionic strength[J].Key Engineering Materials,2002,224-226:631.
[8] Jingtao Ma;Zhipeng Xie;Hezhuo Miao .Elimination of Surface Spallation of Alumina Green Bodies Prepared by Acrylamide-Based Gelcasting via Poly(vinylpyrrolidone)[J].Journal of the American Ceramic Society,2003(2):266-272.
[9] Lewis J.A.;, .Colloidal Processing of Ceramic[J].Journal of the American Ceramic Society,2000(10):2341-2359.
[10] 潘祖仁.高分子化学[M].北京:化学工业出版社,2007:60.
[11] 马利国,黄勇,杨金龙,苏亮,赵雷.凝胶注模成型固化过程及其影响因素--陶瓷浆料凝胶点测定及其影响因素的研究[J].成都大学学报(自然科学版),2002(02):5-10.
[12] L.G. Ma;Y. Huang;J.L. Yang .Control of the inner stresses in ceramic green bodies formed by gelcasting[J].CERAMICS INTERNATIONAL,2006(2):93-98.
[13] 杨金龙,戴春雷,马天,马利国,黄勇.高可靠性陶瓷部件胶态注射成型关键技术及装备[J].中国有色金属学报,2004(z1):243-249.
[14] 杨金龙,马利国,马天,黄勇.陶瓷胶态注射成型液固转变过程中内应力产生机制初探[J].真空电子技术,2003(04):9-12.
[15] Zhang L M;Ma L G;Ma T et al.Origin,transformation and control of the inner stress in the green bodies prepared by ceramic colloidal forming processing[J].Materials Science Forum,2005,475-479:1313.
[16] Abbas E N;Ham Y P;Draskovich B S et al.Physical model for the drying of gelcast ceramics[J].Journal of the American Ceramic Society,1999,82(03):513.
[17] Y. Huang;L.G. Ma;H.R. Le .Improving the homogeneity and reliability of ceramic parts with complex shapes by pressure-assisted gel-casting[J].Materials Letters,2004(30):3893-3897.
[18] 黄勇,张立明,杨金龙,谢志鹏,汪长安,陈瑞峰.先进陶瓷胶态成型新工艺的研究进展[J].硅酸盐学报,2007(02):129-136.
[19] 冯亚青;王利军;陈立功.助剂化学及工艺学[M].北京:化学工业出版社,1997:12.
[20] 何平笙.高聚物的力学性能[M].合肥:中国科学技术大学出版社,1997:117.
[21] Ma L G et al.Effect of plasticizer on the cracking of ceramic green bodies in gelcasting[J].Journal of Materials Science,2005,40(18):4947.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%