The dynamic tensile deformation and fracture behavior of the Zr-based metallic glass/porous W phase composite were investigated at room temperature by means of the Split Hopkinson Tension Bar (SHTB). It was found that the composite exhibited no appreciable macroscopic plastic deformation prior to catastrophic fracture and the fracture surface was perpendicular to the axial direction. Substantive micro cracks were observed along the interface between W grains or the interface between the metallic glass phase and the W phase. Scanning electron microscopy (SEM) observations revealed that vein-like patterns, dimple-like patterns and substantive ridge-like structures were the typical fracture morphologies on the fracture surface for the metallic glass phase and the morphology of the W phase is a mixture of intergranular and transgranular fracture. Based on those results referred above, the dynamic tensile deformation and fracture mechanism of the Zr-based metallic glass/porous W phase composite were discussed in detail.

参考文献

[1] R. D. Conner;A. J. Rosakis;W. L. Johnson;D. M. Owen .Fracture toughness determination for a beryllium-bearing bulk metallic glass[J].Scripta materialia,1997(9):1373-1378.
[2] C. J. Gilbert;R. O. Ritchie;W. k. Johnson .Fracture toughness and fatigue-crack propagation in a Zr-Ti-Ni-Cu-Be bulk metallic glass[J].Applied physics letters,1997(1/4):476-478.
[3] M.Z. Ma;R.P. Liu;Y. Xiao;D.C. Lou;L. Liu;Q. Wang;W.K. Wang .Wear resistance of Zr-based bulk metallic glass applied in bearing rollers[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2004(1/2):326-330.
[4] J. Jayaraj;D. J. Sordelet;D. H. Kim;Y. C. Kim;E. Fleury .Corrosion behaviour of Ni-Zr-Ti-Si-Sn amorphous plasma spray coating[J].Corrosion Science: The Journal on Environmental Degradation of Materials and its Control,2006(4):950-964.
[5] A.Inoue .Stabilization of metallic supercooled liquid and bulk amorphous alloys[J].Acta materialia,2000(1):279-306.
[6] H. CHOI-YIM;R. BUSCH;U. KOSTFR;W. L. JOHNSON .SYNTHESIS AND CHARACTERIZATION OF PARTICULATE REINFORCED Zr57Nb5Al10Cu15.4Ni12.6 BULK METALLIC GLASS COMPOSITES[J].Acta materialia,1999(8):2455-2462.
[7] F. SZUECS;C. P. KIM;W. L. JOHNSON .MECHANICAL PROPERTIES OF Zr_(56.2)Ti_(13.8)Nb_(5.0)Cu_(6.9)Ni_(5.6)Be_(12.5) DUCTILE PHASE REINFORCED BULK METALLIC GLASS COMPOSITE[J].Acta materialia,2001(9):1507-1513.
[8] R.D. Conner;R.B. Dandliker;V. Scruggs .Dynamic deformation behavior of tungsten-fiber/metallic-glass matrix composites[J].International journal of impact engineering,2000(5):435-444.
[9] Z. Bian;G. He;G. L. Chen .Investigation of shear bands under compressive testing for Zr-base bulk metallic glasses containing nanocrystals[J].Scripta materialia,2002(6):407-412.
[10] F.F. Wu;Z.F. Zhang;A. Peker .Strength asymmetry of ductile dendrites reinforced Zr- and Ti-based composites[J].Journal of Materials Research,2006(9):2331-2336.
[11] G. Wang;J. Shen;J.F. Sun .Tensile fracture characteristics and deformation behavior of a Zr-based bulk metallic glass at high temperatures[J].Intermetallics,2005(6):642-648.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%