对应用液态金属冷却(LMC)和高速凝固(HRS)方法制备的叶片状高温合金铸件的铸态组织进行了研究,以比较2种定向凝固方法的优缺点.分别对沿铸件凝固方向不同截面位置处的晶粒取向、一次枝晶间距和γ’相尺寸进行了分析.结果表明,对于HRS铸件的中部截面,枝晶的<001>方向偏离铸件轴向的最大角度在抽拉速率由40 μm/s提高至110 μm/s的过程中不断减小.在70 μm/s的抽拉速度下,LMC铸件中部截面处的中心区域内晶粒的最大偏离角度要大于HRS铸件的相应位置处的偏离角,但是晶粒的整体取向却呈现较HRS铸件更集中的趋势.铸件项部截面处的枝晶组织比中部截面处要粗大,这种现象在HRS铸件中更严重.γ’相尺寸在铸件由叶身位置凝固至平台位置的过程中不断粗化.但当抽拉速率高于70 μm/s时,叶身位置和平台位置之间γ’相尺寸之间的差异在LMC铸件中更小.

参考文献

[1] Reed R C.The Superalloys Fundamentals and Applications[M].Cambridge:Cambridge University Press,2006:1.
[2] Bril Seth B;Pollock T M;Kissinger R D;Bowman R R.Superalloys 2000[M].Warrendale,PA:TMS,2000:3.
[3] Gell M;Sullivan C P;VerSnyder F L;Burke J J,Flemings M C,Gorum A E.Chestnut Hill[M].MA:Brook Hill,1974:141.
[4] Giamei A F;Tschinkel J G .[J].Metallurgical and Materials Transactions,1976,13A:1427.
[5] Elliott A J;Tin S;King W T et al.[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,2004,35A(10):3221.
[6] McLean M.Directionally Solidified Materials for High Temperature Service[M].London:The Metals Society,1983:137.
[7] Souza N D;Ardakani M G;McLean M et al.[J].Metallurgical and Materials Transactions,2000,31A:2877.
[8] Konter M;Kats E;Hofmann N;Pollock T M,Kissinger R D,Bowman R R.Superalloys 2000[M].Warrendale,PA:TMS,2000:189.
[9] Zhang J;Lou L H .[J].Journal of Materials Science and Technology,2007,23(03):289.
[10] Brundidge C L;Miller J D;Pollock T M .[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,2011,42A:2723.
[11] Walton D;Chalmers B .[J].Transactions TMS-AIME,1959,215:447.
[12] Yang X L;Dong H B;Wang W et al.[J].Materials Science and Engineering,2004,386A:129.
[13] Elliott A J;Pollock T M .[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,2007,38A(04):871.
[14] Hunt J D.Solidification and Casting of Metals[M].London:The Metals Society,1979:3.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%