研究了铝镇静钢中B元素的脱溶现象。通过热力学分析可知,在铝镇静钢中B的脱溶形式以BN析出为主。将差热分析方法与热处理和透射电镜观察方法结合,观察到BN以MnS为异质核心从奥氏体中析出,形成BN包覆MnS的复合颗粒,BN的开始析出温度接近1100℃,析出具有C曲线特征,热轧后BN析出不完全,部分B元素仍在钢中固溶。析出最充分的温度在900℃到开始析出温度之间,随冷却速度变化,缓慢冷却条件下在1077℃大量析出。

参考文献

[1] 肖丽俊,郭亚东,刘家琪,仇圣桃,李向阳.硼对低碳铝镇静钢中AlN、MnS析出的影响[J].材料与冶金学报,2006(01):53-56.
[2] Deva A;De S K;Jha B K .Strain hardeuing behavior and cold reducibility of boron-added low-carbon steel[J].Journal of Materials Engineering and Performance,2009,18:109-110.
[3] Lopez-Chipres, E;Mejia, I;Maldonado, C;Bedolla-Jacuinde, A;El-Wahabi, M;Cabrera, JM .Hot flow behavior of boron microalloyed steels[J].Materials Science & Engineering. A, Structural Materials: Properties, Microstructure and Processing,2008(1-2):49-55.
[4] 吴平,贺信莱,王学敏,曹兵,于栋友.冷却-等温-冷却处理过程硼的晶界偏聚[J].材料工程,2001(12):24-28.
[5] Wang M X;He X L .Effect of boron addition on structure and properties of low carbon bainitic steels[J].ISIJ International,2002,42(Su):s38s46.
[6] Jun H J;Kang J S;Seo D H et al.Effects of deformation and boron on microstructure and continuous cooling transformation in low carbon HSLA steel[J].Materials Science and Engineering A,2006,422:157-162.
[7] 赵振华,陈伟庆,袁辉,李永东.硼对低碳钢晶粒尺寸的影响[J].钢铁,2006(03):67-70.
[8] 雍岐龙.钢铁材料中的第二相[M].北京:冶金工业出版社,2006
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%