用热压的方法合成了若干MAX相化合物,包括相(Ti2AlCTi2AlN)和312相(Ti3SiC2Ti3AlC2;研究了它们在1 mol/L HCl1 mol/L NaOH1 mol/L H2SO4中的电化学性质及其结构与其稳定性的关系.结果表明:在所有溶液中,312MAX相比211相更稳定;Ti3SiC2 Ti3AlC2几乎在所有溶液里都发生钝化,而Ti2AlCTi2AlN1 mol/L HCl中活跃地溶解,还伴有大量气泡产生;Ti3SiC2Ti2AlCTi2AlN Ti3AlC2更稳定.

Electrochemical performance was characterized in solutions of 1 mol/L HCl,1 mol/L NaOH and 1 mol/L H2SO4 of several compounds of MAX phase i.e.211phase (Ti2AlC and Ti2AlN) and 312 phase (Ti3SiC2and Ti3AlC2)synthesized by hot pressing.The relation between the structure of MAX phase compounds and their stability was studied in regarding to their electrochemical behavior.It is shown that MAX compounds of 312 phase was more stable than that of 211 phase in all solutions;Ti3SiC2 and Ti3AlC2 could be passivated in all solutions,while Ti2AlC and Ti2AlN underwent active dissolution in 1 mol/L HCl with evolution of gas;Ti3SiC2 was more stable than those of Ti2AlC,Ti2AlN and Ti3AlC2.

参考文献

上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%