A new silver rare earth oxide contact material, Ag/La2O3(12), was produced by powder metallurgy method. Its performances are as follows: the density is 9.71~9.96 g*cm-3; the hardness (HB) is 760~970 MPa and the resistivity is 2.25~2.38 μΩ*cm. The microstructure of Ag/La2O3(12) was analyzed by SEM and EDS. Rare earth oxide La2O3 shows two shapes, which are uniformly distributed in the form of sphere and abnormality in Ag matrix. La2O3 shows fine spherical shape in the melted area of Ag after laser acting which is used to simulate electric arc. The results are contributed to the less splash erosion of Ag. Compared with the main physical and mechanical properties of Ag/SnO2(12) and Ag/CdO(12), the properties of three contact materials are similar, and hence Ag/La2O3(12) may become a potential contact material to be used as the substitute of Ag/CdO(12).

参考文献

[1] Jeannot D;PINARD J .Physical and chemical properties of metal oxide addition to Ag/SnO2 contact materials and predictions of electrical performance[J].IEEE Transactions on Components Packaging and Manufacturing Technology,1994,17(01):17-23.
[2] Mayer V;MICHAL R.Switching behavior and changes in microstructures of silver-metal oxide contact materials[A].Japan,1988:361-367.
[3] WAN Jiang-wen;ZHANG Ji-gao.Adjustment state and quasi steady state of structure and composition of Ag MeO contacts by breaking arcs[A].American,1998:202-206.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%