采用固相反应合成法制备了(1-x)(0.96Bi0.5Na0.5TiO3-0.04BaTiO3)-xBi(Zn0.5 Ti0.5)O3陶瓷(x≤0.10).通过X射线衍射,介电温度谱等对该体系陶瓷的相结构及弛豫特性进行了研究.结果发现,该陶瓷在Bi(Zn0.5Ti05)O3加入量低于0.05时呈现纯钙钛矿结构.此外,随着Bi(Zn0.5Ti0.5)O3加入量的增加,其相结构由三方-四方共存向赝立方结构转变;同时,陶瓷的弥散因子上升,偶极子取向冻结活化能下降,表明BZT的加入明显地增加了0.96Bi0.5Na0.5TiO3-0.04 BaTiO3陶瓷的弛豫性.

参考文献

[1] 高龙,杨世源,王进,郭学,钱斌.多孔PZT 95/5铁电陶瓷的孔隙率与电性能[J].人工晶体学报,2013(03):446-451.
[2] 江向平,古训玖,张凯韦,陈超,李小红,涂娜.Na0.5Bi0.5TiO3-K0.5Bi0.5TiO3-BaMnO3无铅压电陶瓷的结构与电性能[J].人工晶体学报,2012(04):916-921.
[3] 李晓娟,惠增哲,龙伟,方频阳.不同离子掺杂的钛酸铋钠基陶瓷结构与性能表征[J].人工晶体学报,2013(11):2346-2350.
[4] Vladimir V. Shvartsman;Doru C. Lupascu .Lead-Free Relaxor Ferroelectrics[J].Journal of the American Ceramic Society,2012(1):1-26.
[5] Grinberg I;Suchomel MR;Dmowski W;Mason SE;Wu H;Davies PK;Rappe AM .Structure and polarization in the high T-c ferroelectric Bi(Zn,Ti)O-3-PbTiO3 solid solutions[J].Physical review letters,2007(10):7601-1-7601-4-0.
[6] Shan-Tao Zhang;Feng Yan;Bin Yang .Morphotropic phase boundary and electrical properties in (1-x)Bi_(0.5)Na_(0.5)TiO_(3)-xBi(Zn_(0.5)Ti_(0.5))O_(3) lead-free piezoceramics[J].Journal of Applied Physics,2010(11):114110-1-114110-4.
[7] Ruzhong Zuo;Yi Liu;Shi Su .Phase Transformation Behavior and Electrical Properties of Pb(Zr_(0.56)Ti_(0.44))O_3-Bi(Zn_(0.5)Ti_(0.5))O_3 -Solid -Solution -Ceramics[J].Journal of the American Ceramic Society,2011(12):4340-4344.
[8] YUJI HIRUMA;KAZUSHIGE YOSHII;HAJIME NAGATA .Investigation of Phase Transition Temperatures on (Bi_(1/2)Na_(1/2))TiO_3-(Bi_(1/2)K_(1/2))TiO_3 and (Bi_(1/2)Na_(1/2))TiO_3-BaTiO_3 Lead-free Piezoelectric Ceramics by Electrical Measurements[J].Ferroelectrics: Letters Section,2007(1):114-119.
[9] Wang, F.;Xu, M.;Wang, T.;Tang, Y.;Shi, W. .Phase transition and electrical properties in the Li-modified Bi _(0.5)Na _(0.5)TiO _3-based lead-free ceramics[J].Journal of Materials Science,2012(5):2352-2358.
[10] 刘立英,侯育冬,朱满康,王波,严辉.(Na0.5Bi0.5)TiO3基弛豫铁电体相变的研究进展[J].材料导报,2005(08):17-19,24.
[11] 初宝进,李国荣,江向平,陈大任.Na1/2Bi1/2TiO3-BaTiO3系陶瓷压电性?及弛豫相变研究[J].无机材料学报,2000(05):815-821.
[12] Mankang Zhu;Hancheng Hu;Na Lei;Yudong Hou;Hui Yan .Dependence of depolarization temperature on cation vacancies and lattice distortion for lead-free 74(Bi_(1/2)Na_(1/2))TiO_(3)-20.8(Bi_(1/2)K_(1/2))TiO_(3)-5.2BaTiO_(3) ferroelectric ceramics[J].Applied Physics Letters,2009(18):182901-1-182901-3-0.
[13] 张绍锋,李强,杨子.准同型相界组分PMNT弛豫铁电单晶的畴结构与极化特性[J].人工晶体学报,2009(02):411-415.
[14] WU NingNing,SONG XueMei,HOU YuDong,ZHU ManKang,WANG Chao YAN Hui.Relaxor behavior of (1-x)Pb(Mg1/3Nb2/3)O3-xPbTiO3 ceramics[J].科学通报(英文版),2009(07):1267-1274.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%