研究了NZ2锆合金板材在不同温度、不同浓度的碘蒸气中的力学行为,并进一步通过扫描电镜观察其断口形貌.结果表明,试验温度为400℃,其发生应力腐蚀的临界碘蒸气压约为102 Pa;横向试样较轧向试样更具应力腐蚀敏感性;温度升高能够促进裂纹尖端的应力释放,有利于碘能被更有效地吸附到裂纹尖端,加快对锆合金的腐蚀作用,从而降低了应力腐蚀的临界碘浓度.在高温碘蒸气中,断口腐蚀产物主要为锆的氧化物;虽然碘蒸气对锆有较强的腐蚀作用,但是不足以穿透其表面的保护膜,而局部变形则可以促进碘对金属锆的腐蚀.

参考文献

[1] Gwenn Lelievre;Daniel Fruchart;Pierre Convert .Characterisation by neutron diffraction in high temperature pressurised water of the surface corrosion and hydrogen embrittlement of zircaloy-4[J].Journal of Alloys and Compounds: An Interdisciplinary Journal of Materials Science and Solid-state Chemistry and Physics,2002(1/2):288-294.
[2] Goryachev S B;Gritsuk A R et al.[J].Journal of Nuclear Materials,1992,199:50.
[3] Peehs M;Stehle H;Steinberg E.[A].Philadelphia:ASTM STP681,1979:244.
[4] Woo Seog Ryu;Young Hwan Kang;Jai-Young Lee .[J].Journal of Nuclear Materials,1988,152:194.
[5] Sidky P S .[J].Journal of Nuclear Materials,1998,256:1.
[6] Fregonese M;Florence Lefebver;Clement Lemaignan et al.[J].Journal of Nuclear Materials,1999,265:245.