采用恒电位极化法测定了电阻焊油井套管经过模拟热张力减径处理试验后的沟槽腐蚀性能。结果表明,电阻焊管母材和焊缝区的微观组织差异及焊缝区的应力是电阻焊管沟槽腐蚀的主要原因。热张力减径可以显著提高电阻焊油井套管的抗沟槽腐蚀性能,从而扩大其在石油钻采领域的应用。

The grooving corrosion performance of electric resistance welded (ERW) oil well casing after simulation of thermal tension reduction process was investigated by potentiostatic polarization method. It was found that the microstructure difference between base metal and weld zone and the stress in weld zone were two main causes of grooving corrosion of ERW tube. The thermal tension reduction process can considerably improve the grooving corrosion resistibility of ERW oil well casing. And the ERW tube can be used more in the field of oil drilling.

参考文献

[1] 李平.油水集输管线中沟槽腐蚀成因分析[J].材料保护,1993(06):6.
[2] 王荣.J55钢直缝焊油井套管沟槽腐蚀性能研究[J].中国腐蚀与防护学报,2004(06):360-363.
[3] 李鹤林.油井管发展动向及若干热点问题(上)[J].钢管,2005(06):1-6.
[4] 介升旗,刘永平.国内ERW焊管发展现状及其质量控制[J].焊管,2006(06):74-79.
[5] 范丽霞,卢卓宇,任峰,蒋昌忠,付强.EBSD在InGaAsP/InP异质结构弹性应力区域的研究[J].武汉理工大学学报,2007(z1):39-41.
[6] 黄亚敏,潘春旭.基于电子背散射衍射(EBSD)技术的材料微区应力应变状态研究综述[J].电子显微学报,2010(01):1-11.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%