Research status of high strength low alloy TRIP (transformation induced plasticity) steels for automobile structural parts is briefly described. Composition and microstructure factors especially the morphology, size and volume fraction of retained austenite,which largely influence the strength and ductility of the steel, are reviewed and discussed one after another. Modelling of the inter-critical annealing and martempering processes as well as the designing of the TRIP steel aided by commercial software are introduced. Some special aspects of the dynamic mechanical properties of TRIP steel are firstly reported.
关键词:
张清
,
李全安
,
井晓天
,
张兴渊
材料工程
doi:10.3969/j.issn.1001-4381.2011.03.016
Mg24Y5相的细化是进一步提高Mg-l0Y合金力学性能的关键.研究了稀土元素sm对Mg-l0Y合金中的Mg24Y5相及其基体组织的细化作用,结果表明:sm的加人,改善了Mg24Y5相的形貌,促进了细小弥散分布的Mg24Y5颗粒相的形成;同时,Sm的加人,通过固溶作用,进一步细化了基体组织;显微组织的改善导致了合金高温下力学性能的提高.
关键词:
Sm
,
Mg-10Y合金
,
组织细化
,
力学性能
ZHANG Lei WANG Peixuan TAO Rong MA Ruzhang ZHANG Guoguang University of Science and Technology Beijing
,
Beijing
,
China professor
,
Department of Materials Physics.University of Science and Technology Beijing.Beijing 100083
,
China
金属学报(英文版)
Nucleation and growth of He bubbles at different annealing temperatures T≤1023 K in stain- less steels HR-2 and SS321,implanted with He~+(40-70 keV.1×10~(16)-6× 10~(17) He~+/cm~2),were ohserved under TEM.T=0.45T_m seems to be a transition temperature.The He bubbles continue mainly their nucleation at 0.3T_m< T<0.45T_m,and grow predominantly at T≥0.45T_m,due probably to migration and coalescence by surface diffusion of metal atoms around the bubbles.The apparent activation energies for the growth are found to he 0.41 and 0.31 eV for HR-2 and SS321 respectively.The bubble density in HR-2 is greater than that in SS321 within whole measuring temperature range,and the onset temperature of rapid swelling is also higher.It is believed that the resistance of HR-2 to He is superior to that fo SS321.
关键词:
stainless steel
,
null
,
null
,
null
,
null
Journal of Nuclear Materials
Due to its inert reactivity with almost elements, He-3 produced from tritium decay has extremely detrimental effects on the tritide. To refrain from this He-3-induced damage, an efficient way is to increase the stability of He-3 in metal tritide by alloying. Using a first-principles discrete variational method in two cluster models, one for a low He-3 concentration and the other for a high He-3 concentration, the authors study the alloying effect of 3d and 4d transition metals on the stability of He-3 in TiT2 system. It is found that the preferring and metastable sites of He-3 are affected by He-3 concentration : He-3 prefers to stay at original tetrahedral interstitial site when He-3 concentration is low but moves to octahedral site when He-3 concentration is high enough. A criterion of alloying effect is proposed, according to which Nb, Y, Zr, Pd, Ru, Tc, Rh, Cr, Mo and Ag are suggested to be the beneficial alloying elements for increasing the stability of He-3 in the alloyed TiT2 with a low He-3 concentration and Y, Nb, Mo, Zr, Cr, Tc, Ru, Rh and Cu for that with a high He-3 concentration. Our results of alloying effect are supported by the positron annihilation spectroscopy (PAS) measurements for He-implanted Ti, TiMoYAl and TiZrYAl films. (c) 2006 Elsevier B.V. All rights reserved.
关键词:
electronic population analysis;molecular wave functions;hydrogen;storage alloys;intermetallic hydride;bubble formation;iron clusters;helium;tritides;lcao;overlap
李悦
,
邓爱红
,
刘莉
,
王康
,
谢莎
材料研究学报
利用x射线衍射(xRD)和慢正电子束分析(SPBA)技术研究高温退火后含He钛膜的微观结构和钛膜内He相关缺陷的演化.XRD分析表明,高温退火后Ti和Si在高温下发生反应形成稳定的多晶TiSi2化合物,He原子的掺入会影响TiSi2晶体的择优取向,而对TiSi2晶粒尺寸的影响较小.SPBA结果表明,室温下,钛膜内的缺陷浓度或尺寸会随着掺He浓度的增加而增大;高温退火后,当He浓度小于5%(原子分数,下同)时(除2%外),钛膜内的He相关缺陷浓度随着He浓度增加相应地增加.当He浓度增加到14%时,高温会使较高浓度的He原子、He-空位复合体以及小He泡迁移聚集形成一些尺寸较大He泡,而较大He泡周围与He相关的小尺寸缺陷的浓度则会发生相应地减少.
关键词:
金属材料
,
含He钛膜
,
直流磁控溅射
,
He相关缺陷
,
XRD
,
SPBA
施立群
,
金钦华
,
刘超卓
,
徐世林
,
周筑颖
原子核物理评论
doi:10.3969/j.issn.1007-4627.2005.01.045
研究了用He/Ar混合溅射气体的直流磁控溅射制备钛膜中He的掺入现象.分析结果表明,大量的He原子(He/Ti原子比高达56%) 被均匀地引入到Ti膜中,He含量可由混合溅射气体的He分量精确控制.通过调节溅射参数,可实现样品中He的低损伤引入.研究还发现,溅射沉积的含氦Ti膜具有较高的He成泡剂量和高的固He能力,这可能是溅射沉积形成了纳米晶Ti膜所致.纳米晶Ti膜较粗晶材料具有很高浓度的He捕陷中心,使He泡密度增大而泡尺寸减小.随He引入量的增加,Ti膜的晶粒尺寸减小,He引起的晶体点阵参数和X射线衍射峰宽度增大,晶体的无序程度增加.
关键词:
氦
,
损伤
,
泡
,
钛膜
,
溅射沉积
贺建超
,
高进
,
邓东
,
万发荣
材料工程
doi:10.11868/j.issn.1001-4381.2016.04.015
研究辐照下He在氧化物弥散强化材料中小于5nm的氧化物颗粒的稳定性.在有He环境下,对14YWT氧化物弥散强化材料进行高温离子辐照.采用三维原子探针(APT)对辐照前后样品中的氧化物颗粒的大小、密度、成分以及其空间分布进行分析.结果表明:小于5 nm的弥散氧化物颗粒主要是由Y和Ti的氧化物组成,在辐照前后其成分、尺寸和空间分布无明显变化,说明在600℃高温重离子辐照过程中,在有He环境下铁素体ODS材料中弥散氧化物颗粒仍具有良好的稳定性.
关键词:
氧化物弥散强化材料
,
辐照
,
纳米氧化物颗粒
,
稳定性
丁兆勇
,
孙保民
,
刘远超
,
许秉浩
人工晶体学报
在用热解火焰法合成碳纳米管(carbon nanotubes, CNTs)过程中,CO、H2和He流量对产物种类以及CNTs的产量、结构、管径、管长等有显著影响.为了确定CO、H2和He流量的具体影响,通过固定其他实验条件,仅改变CO、H2和He流量,用扫描电子显微镜(SEM)和高分辨率透射电子显微镜(HR-TEM)对合成的产物进行表征,分析得到合成CNTs较好的CO、H2和He流量分别为0.4 L/min,0.3 L/min和0.2 L/min.
关键词:
碳纳米管
,
流量
,
热解火焰
,
SEM
,
TEM