DETERMINATION OF PrCl_3-NaCl-LiCl PHASE DIAGRAM

QIAO Zhiyu WANG Mingsheng ZHENG Chaogui DUAN Shuzhen University of Science and Technology Beijing , Beijing , China Qiao Zhiyu , Professor , Dept.of Physical Chemistry University of Science and Technology Beijing , 30 Xueyuan Road , Beijing 100083 , China

金属学报(英文版)

PrCl_3-NaCl-LiCl phase diagram has been constructed from the phase diagrams of its sub-binary systems and of six quasi-binary systems measured by DTA technique.It is found that this ternary system is composed of five liquidus surfaces,seven second crystallization lines,two peritectic points and one eutectie point.The temperatures and compositions of invariant points are as follows:P_1(416℃,30.3 mol% NaCl,44.2 mol% LiCl,25.5 mol% PrCl_3);P_2(409℃,25.0 mol% NaCl,50.0 mol% LiCl,25.0 mol% PrCl_3);E(404℃,20.0 mol% NaCl,55.4 mol% LiCl,24.6 mol% PrCl_3).

关键词: PrCl_3-NaCl-LiCl , null , null

CORRELATION BETWEEN STRESS COMPONENTS AND STRESS CORROSION CRACKS IN BRASS Lecturer,Department of Materials Physics,University of Science and Technology Beijing,Beijing 100083,China

QIAO Lijie LIU Rui XIAO Jimei University of Science and Technology Beijing , Beijing , China

金属学报(英文版)

The effects of stress components on nucleation sites and propagation directions of stress cor- rosion cracks in brass were investigated with specimens under mode Ⅱ and mode Ⅲ loadings. The results indicated that under mode Ⅱ loading,stress corrosion cracks nucleated on the site with maximum normal stress component and propagated along the plane perpendieular to the maximum normal stress,under mode Ⅲ loading,the stress corrosion crack was not evident on the 45°plane due to the general corrosion in aqueous solution with high NH_4OH concentra- tion,while stress corroded in aqueous solution with low NH_4OH concentration, numerous cracks with spacings of 10—150μm were found on the 45°plane with maximum normal stress and no stress corrosion cracks was observed on the plane with maximum shear stress.

关键词: stress corrosion cracking , null , null , null

Physical Simulation of New Desulphurization Technology Using Pulsed and Rotary StirringInjection

WU Wei , WU Wei , HU Yanbin , LIU Liu , DING Yongliang

钢铁研究学报(英文版)

The contrast experiment of different stirring modes, which includes a new type of stirringinjection with the method of pulse and rotation, and the initial oneway stirring method, is done through physical simulation in the laboratory. The stirring methods of pulse and rotation are of two kinds. One is pulsed and rotary stirrer with positive and opposite directions. The other is pulsed and rotary stirrer with rotationstoprotation. The results show that the stirring mode of pulse and rotation has better effects than the oneway stirring method. The specific effects are that the mixing time of the melting bath is apparently shortened, the number of grains involved in the liquid surface is increased, and the residence time of air bubble in water is doubled.

关键词: hot metal;desulphurization;injection;physical simulation;pulse;rotation